Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Teijin Films Melinex® 534 Polyester Film, 380 Gauge

Category Polymer , Film , Thermoplastic , Polyester, TP , Polyester Film
Manufacturer DuPont Teijin Films (DTF)
Trade Name Melinex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Teijin Films Melinex® 534 Polyester Film, 380 Gauge.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Melinex® 534 is an opaque white film with superb handling properties and a unique glossy appearance. It is pre-treated on both surfaces to promote adhesion to aqueous based inks and coatings.Information provided by DuPont.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 161 MPa
23400 psi
ASTM D882A
Film Tensile Strength at Yield, TD 85.5 MPa
12400 psi
ASTM D882A
Film Elongation at Break, MD 152 %
152 %
ASTM D882A
Film Elongation at Break, TD 105 %
105 %
ASTM D882A
Coefficient of Friction, Dynamic 0.32
0.32
A-B; ASTM D1894
Film Tensile Strength at Break, MD 138 MPa
20000 psi
ASTM D882A
Film Tensile Strength at Break, TD 85.5 MPa
12400 psi
ASTM D882A
Thermal Properties Metric English Comments
Shrinkage, MD 0.70 %

@Temperature 190 °C,
Time 300 sec
0.70 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Shrinkage, TD 0.60 %

@Temperature 190 °C,
Time 300 sec
0.60 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Optical Properties Metric English Comments
Transmission, Visible 13 %
13 %
TLT; ASTM D1003
Descriptive Properties Value Comments
Yield (nominal) 5200 in2/lb
Copyright © lookpolymers.com All Rights Reserved