Material Notes:
Melinex® 542 is a slightly hazy film with an adhesion promoting pretreatment on both sidesGeneral Product Info: The pretreatment enables numerous solvent and UV inks and lacquers to be coated with excellent adhesion. The film is tear resistant, has excellent handling characteristics and also good dimensional stability when exposed to variations in temperature and humidity.Typical Applications: This film was primarily developed for use in the Reprographics industry.Approvals: UL Recognition - Product has been registered with Underwriters LaboratoriesInformation provided by DuPont.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 193 MPa
28000 psi
50% strain rate; ASTM D882A
Film Tensile Strength at Break, TD 255 MPa
37000 psi
50% Strain rate; ASTM D882A
Thermal Properties Metric English Comments
Melting Point 255 - 260 °C
491 - 500 °F
ASTM E794-85
Shrinkage, MD 2.5 %

@Temperature 190 °C,
Time 300 sec
2.5 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Shrinkage, TD 0.50 %

@Temperature 190 °C,
Time 300 sec
0.50 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Optical Properties Metric English Comments
Haze <= 9.0 %

@Thickness 0.0361 mm
<= 9.0 %

@Thickness 0.00142 in
Gardner Hazemeter; ASTM D1003-77
<= 13 %

@Thickness 0.0500 mm
<= 13 %

@Thickness 0.00197 in
Gardner Hazemeter; ASTM D1003-77
<= 14 %

@Thickness 0.0752 mm
<= 14 %

@Thickness 0.00296 in
Gardner Hazemeter; ASTM D1003-77
<= 23 %

@Thickness 0.100 mm
<= 23 %

@Thickness 0.00394 in
Gardner Hazemeter; ASTM D1003-77
<= 26 %

@Thickness 0.125 mm
<= 26 %

@Thickness 0.00493 in
Gardner Hazemeter; ASTM D1003-77