Material Notes:
Melinex® 583 is a high clarity, differentially treated polyester film. One side is hydrophilic pretreated to promote adhesion to many industrial aqueous coatings and inks, and the opposite side is pretreated for antistatic protection.Information provided by DuPont.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 100 MPa

@Strain >=5.00 %
14500 psi

@Strain >=5.00 %
ASTM D882A
Film Elongation at Break, MD 170 %
170 %
ASTM D882A
Film Elongation at Break, TD 120 %
120 %
ASTM D882A
Coefficient of Friction, Dynamic 0.50
0.50
A-B; ASTM D1894
Film Tensile Strength at Break, MD 193 MPa
28000 psi
ASTM D882A
Film Tensile Strength at Break, TD 241 MPa
35000 psi
ASTM D882A
Thermal Properties Metric English Comments
Shrinkage, MD 2.5 %

@Temperature 190 °C,
Time 300 sec
2.5 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Shrinkage, TD 1.0 %

@Temperature 190 °C,
Time 300 sec
1.0 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Optical Properties Metric English Comments
Haze 1.0 %
1.0 %
ASTM D1003
Transmission, Visible 90 %
90 %
TLT; ASTM D1003
Electrical Properties Metric English Comments
Surface Resistivity per Square 1.60e+11 ohm

@Temperature 25.0 °C
1.60e+11 ohm

@Temperature 77.0 °F
500 V DC @ 66% RH; ASTM D257