DuPont Teijin Films Mylar® 834 Polyester Film, 48 Gauge

Category Polymer , Film , Thermoplastic , Polyester, TP , Polyester Film
Manufacturer DuPont Teijin Films (DTF)
Trade Name Mylar®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Teijin Films Mylar® 834 Polyester Film, 48 Gauge.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Mylar® 834 is a packaging grade polyester film, chemically pretreated on one side for controlled COF and release.Approvals: FDA Food Contact Status - All gauges of Mylar® 834 comply with the Food and Drug Administration regulation 21 CFR 177.1630 -- Polyethylene phthalate polymers. This regulation describes films which may be safely used in contact with all types of food excluding alcoholic beverages. Mylar® 834 can be used to contain foods during oven cooking or oven baking at temperatures above 250°F.Information provided by DuPont.
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 110 %
110 %
ASTM D882A
Film Elongation at Break, TD 70 %
70 %
ASTM D882A
Coefficient of Friction, Static 0.30
0.30
ASTM D1894
Film Tensile Strength at Break, MD 222 MPa
32200 psi
ASTM D882A
Film Tensile Strength at Break, TD 269 MPa
39000 psi
ASTM D882A
Thermal Properties Metric English Comments
Specific Heat Capacity 1.17 J/g-°C
0.280 BTU/lb-°F
Typical Mylar®
Melting Point 254 °C
489 °F
Typical Mylar® via DSC
Maximum Service Temperature, Air 121 °C
250 °F
Optical Properties Metric English Comments
Refractive Index 1.64 - 1.67
1.64 - 1.67
typical of Mylar®
Haze 3.6 %
3.6 %
ASTM D1003
Descriptive Properties Value Comments
Yield (nominal) 42200 in2/lb