Material Notes:
Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, and processability.Mylar® A films have balanced tensile properties and excellent resistance to moisture and most chemicals. They can withstand temperature extremes from -100°F to 300ºF. Mylar® does not become brittle with age under normal conditions, because it contains no plasticizers. Typical Applications:Apparel staysBook jacketsCarbon ribbonControl TapeDrumheadsDuct LinersIdentificationsMembrane touch switchesMetallized BasePressure Sensitive Labels (plain or metallized)Protective surfacingRelease linersRoll leaf (hot stamping)Spirit MastersApprovals: FDA Food Contact Status - All gauges of Mylar® A comply with the Food and Drug Administration regulation 21 CFR 177.1630 -- Polyethylene phthalate polymers. This regulation describes films which may be safely used in contact with all types of food excluding alcoholic beverages. Uncoated films such as Mylar® A can be used to contain foods during oven cooking or oven baking at temperatures above 250 °F. UL 94 VTM-2 - for 92-1400 gauge (0.023 - 0.35mm). UL Recognition - for 92-500 gauge (0.023-0.13mm) HWI=5, HAI=4, CTI=1; for 700-1400 gauge (0.18-0.35mm) HWI=4, HAI=0, CTI=1Information provided by DuPont.
Physical Properties Metric English Comments
Density 1.39 g/cc
0.0502 lb/in³
ASTM D1505
Viscosity Measurement 0.56
0.56
ASTM D2857
Mechanical Properties Metric English Comments
Tensile Modulus 3.50 GPa
507 ksi
ASTM D822
Poissons Ratio 0.38
0.38
Typical Mylar® before yield
0.58
0.58
Typical Mylar® after yield
Thermal Properties Metric English Comments
CTE, linear 17.0 µm/m-°C

@Temperature 30.0 - 50.0 °C
9.44 µin/in-°F

@Temperature 86.0 - 122 °F
92 Gauge; ASTM D696
Specific Heat Capacity 1.17 J/g-°C
0.280 BTU/lb-°F
Thermal Conductivity 0.155 W/m-K

@Temperature 25.0 - 75.0 °C
1.07 BTU-in/hr-ft²-°F

@Temperature 77.0 - 167 °F
(Mylar® 1000A)
Melting Point 254 °C
489 °F
DSC
Maximum Service Temperature, Air 149 °C
300 °F
Maximum Service Temperature, Inert -73.3 °C
-100 °F
Optical Properties Metric English Comments
Refractive Index 1.64 - 1.67
1.64 - 1.67
typical of Mylar®
Electrical Properties Metric English Comments
Comparative Tracking Index 400 - 600 V
400 - 600 V
Hot Wire Ignition, HWI 7.0 - 15 sec
7.0 - 15 sec
High Amp Arc Ignition, HAI >= 120 arcs
>= 120 arcs