Material Notes:
Mylar® ADS is a heat stabilized, low shrinkage film with good web handling properties. Approvals: UL 94 VTM-2 - for 92 - 500 gauge (0.023 - 0.13mm)Also available in 285 GaugeInformation provided by DuPont.
Physical Properties Metric English Comments
Density 1.39 g/cc
0.0502 lb/in³
Typical Mylar®; ASTM D1505
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 160 %
160 %
ASTM D882A
Film Elongation at Break, TD 140 %
140 %
ASTM D882A
Film Tensile Strength at Break, MD 173 MPa
25100 psi
ASTM D882A
Film Tensile Strength at Break, TD 188 MPa
27300 psi
ASTM D882A
Thermal Properties Metric English Comments
Specific Heat Capacity 1.17 J/g-°C
0.280 BTU/lb-°F
Typical Mylar®
Melting Point 254 °C
489 °F
Typical Mylar® via DSC
Shrinkage, MD 0.50 %

@Temperature 150 °C,
Time 1800 sec
0.50 %

@Temperature 302 °F,
Time 0.500 hour
Unrestrained
Shrinkage, TD 0.20 %

@Temperature 150 °C,
Time 1800 sec
0.20 %

@Temperature 302 °F,
Time 0.500 hour
Unrestrained
Optical Properties Metric English Comments
Refractive Index 1.64 - 1.67
1.64 - 1.67
typical of Mylar®
Haze 43 %
43 %
ASTM D1003
Electrical Properties Metric English Comments
Dielectric Strength 132.9 kV/mm
3375 kV/in
1/4" electrode 500 V/sec 25°C in air; ASTM D149
Dielectric Breakdown 13500 V
13500 V
1/4" electrode 500 V/sec 25°C in air; ASTM D149