Material Notes:
Mylar® HR951 is a one-side release coated polyester film with good handling properties and clarity. It has been developed for use in various industrial applications.Information provided by DuPont.
Physical Properties Metric English Comments
Density 1.39 g/cc
0.0502 lb/in³
Typical Mylar®; ASTM D1505
Coating Weight 0.0720 g/m²
0.0450 lb/ream
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 140 %
140 %
ASTM D882A
Film Elongation at Break, TD 110 %
110 %
ASTM D882A
Film Tensile Strength at Break, MD 193 MPa
28000 psi
ASTM D882A
Film Tensile Strength at Break, TD 234 MPa
34000 psi
ASTM D882A
Heat Seal Strength >= 22.0 g/25 mm
>= 0.0485 lb/in
using Tesa 7475 Tape
Thermal Properties Metric English Comments
Specific Heat Capacity 1.17 J/g-°C
0.280 BTU/lb-°F
Typical Mylar®
Melting Point 254 °C
489 °F
Typical Mylar® via DSC
Shrinkage, MD 2.5 %

@Temperature 150 °C,
Time 1800 sec
2.5 %

@Temperature 302 °F,
Time 0.500 hour
Unrestrained
Shrinkage, TD 0.50 %

@Temperature 150 °C,
Time 1800 sec
0.50 %

@Temperature 302 °F,
Time 0.500 hour
Unrestrained
Optical Properties Metric English Comments
Refractive Index 1.64 - 1.67
1.64 - 1.67
typical of Mylar®
Haze 2.5 %
2.5 %
ASTM D1003