DuPont Teijin Films Mylar® OWF Polyester Film, 120 Gauge

Category Polymer , Film , Thermoplastic , Polyester, TP , Polyester Film
Manufacturer DuPont Teijin Films (DTF)
Trade Name Mylar®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Teijin Films Mylar® OWF Polyester Film, 120 Gauge.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: Mylar® OWF is a co-extruded, one side amorphous, heat sealable polyester film designed to be used as an overwrap film. This film is suitable for use in contact with food. Approvals: FDA Food Contact Status - All gauges of Mylar® OWF comply with the Food and Drug Administration regulation 21 CFR 177.1630 -- Polyethylene phthalate polymers. This regulation describes films which may be safely used in contact with all types of food excluding alcoholic beverages. Uncoated films such as Mylar® OWF can be used to contain foods during oven cooking or oven baking at temperatures above 250 °F.Information provided by DuPont.
Physical Properties Metric English Comments
Density 1.39 g/cc
0.0502 lb/in³
Typical Mylar®; ASTM D1505
Thermal Properties Metric English Comments
Specific Heat Capacity 1.17 J/g-°C
0.280 BTU/lb-°F
Typical Mylar®
Melting Point 254 °C
489 °F
Typical Mylar® via DSC
Maximum Service Temperature, Air 121 °C
250 °F
Shrinkage, MD 1.5 %

@Temperature 150 °C,
Time 1800 sec
1.5 %

@Temperature 302 °F,
Time 0.500 hour
Unrestrained
Shrinkage, TD 1.5 %

@Temperature 150 °C,
Time 1800 sec
1.5 %

@Temperature 302 °F,
Time 0.500 hour
Unrestrained
Optical Properties Metric English Comments
Haze 6.0 %
6.0 %
ASTM D1003
Transmission, Visible 88.5 %
88.5 %
ASTM D1003
Descriptive Properties Value Comments
Yield (nominal) 16500 in2/lb