DuPont Teijin Films Mylar® XG2 Polyester Film, 92 Gauge

Category Polymer , Film , Thermoplastic , Polyester, TP , Polyester Film
Manufacturer DuPont Teijin Films (DTF)
Trade Name Mylar®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Teijin Films Mylar® XG2 Polyester Film, 92 Gauge.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Mylar® XG2 is an economical film substrate with good handling characteristics for use in thin, clear film applications such as post lamination or silicone release applications. The product is not pretreated on either side.Information provided by DuPont.
Physical Properties Metric English Comments
Density 1.39 g/cc
0.0502 lb/in³
Typical Mylar®; ASTM D1505
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 170 %
170 %
ASTM D882A
Film Elongation at Break, TD 130 %
130 %
ASTM D882A
Coefficient of Friction, Static 0.41
0.41
ASTM D1894
Film Tensile Strength at Break, MD 248 MPa
36000 psi
ASTM D882A
Film Tensile Strength at Break, TD 283 MPa
41000 psi
ASTM D882A
Thermal Properties Metric English Comments
Specific Heat Capacity 1.17 J/g-°C
0.280 BTU/lb-°F
Typical Mylar®
Melting Point 254 °C
489 °F
Typical Mylar® via DSC
Shrinkage, MD 3.0 %

@Temperature 190 °C,
Time 300 sec
3.0 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Shrinkage, TD 1.1 %

@Temperature 190 °C,
Time 300 sec
1.1 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Optical Properties Metric English Comments
Haze 1.8 %
1.8 %
ASTM D1003