Dynasol Solprene® 9340 Multi-branched Thermoplastic Rubber (Multi-branched SBS)

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Dynasol
Trade Name Solprene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dynasol Solprene® 9340 Multi-branched Thermoplastic Rubber (Multi-branched SBS).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Solprene® 9340 is a 66/34 Butadiene-Styrene multi arm copolymer, polymerized in solution process. It has a non-staining FDA approved antioxidant system for food contact applications and it is essentially gel free polymer. This product is presented as a free flowing porous pellet for easy handling and dissolution. Uses: Solprene® 9340 was developed to be used in high performance adhesive formulations. Additionally, it is used as plastic impact modifier and asphalt elastomeric modifier in paving and roofing application.Main Applications: PavingPolymer modificationAdhesivesRoofingInformation provided by Dynasol.
Physical Properties Metric English Comments
Volatiles <= 0.75 %
<= 0.75 %
ASTM D5668
Brookfield Viscosity 950 cP
950 cP
25% in toluene; ASTM D2994
Mechanical Properties Metric English Comments
Hardness, Shore A 71
71
DIN 53505
Tensile Strength 11.8 MPa
1710 psi
ASTM D412
Elongation at Break 925 %
925 %
ASTM D412
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -89.0 °C
-128 °F
ASTM E-1356
Chemical Properties Metric English Comments
Styrene Content >= 32 %
>= 32 %
Block; NM 202-07
34 %
34 %
ASTM D5775