Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

E-Polymers TEKAPPO® JF101 Filler Reinforced Heat Resistant Dimensional Stability Flame Retardant M-PPO

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO
Manufacturer E-Polymers Co. Ltd.
Trade Name TEKAPPO®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF E-Polymers TEKAPPO® JF101 Filler Reinforced Heat Resistant Dimensional Stability Flame Retardant M-PPO.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Modified PPO/PPE: TEKAPPO is a modified PPO/PPE, blending PPO with HIPS in order to improve HDT and processability. It displays various HDT range with halogen-free flammability, impact resistance and reinforced fiberglass. It shows high dimensional stability and rigidity used for housing and electrical parts.Information Provided by E-Polymers Co., Ltd.
Physical Properties Metric English Comments
Specific Gravity 1.22 g/cc
1.22 g/cc
ASTM D792
Water Absorption 0.060 %

@Time 86400 sec
0.060 %

@Time 24.0 hour
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
Linear Mold Shrinkage, Transverse 0.0045 cm/cm
0.0045 in/in
Mechanical Properties Metric English Comments
Tensile Strength 55.917 MPa
8110.1 psi
ASTM D638
Elongation at Break 4.0 %
4.0 %
ASTM D638
Flexural Strength 103.01 MPa
14940 psi
ASTM D790
Flexural Modulus 4.199 GPa
609.0 ksi
ASTM D790
Izod Impact, Notched 0.539 J/cm
1.01 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 100 °C
212 °F
ASTM D648
Flammability, UL94 V-1
V-1
Processing Properties Metric English Comments
Melt Temperature 240 - 300 °C
464 - 572 °F
Mold Temperature 50.0 - 80.0 °C
122 - 176 °F