E-Polymers Tekaloy® T80HI Impact Resistance PBT/ABS Alloy

Category Polymer , Thermoplastic , ABS Polymer , ABS/Polyester Alloy , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer E-Polymers Co. Ltd.
Trade Name TEKALOY®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF E-Polymers Tekaloy® T80HI Impact Resistance PBT/ABS Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Impact ResistanceInformation provided by E-Polymers Co. Ltd.
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0080 cm/cm
0.0080 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Yield 45.0 MPa
6530 psi
ASTM D638
Elongation at Break >= 100 %
>= 100 %
ASTM D638
Flexural Yield Strength 60.0 MPa
8700 psi
ASTM D790
Flexural Modulus 1.90 GPa
276 ksi
ASTM D790
Izod Impact, Notched 6.20 J/cm
11.6 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 89.0 °C
192 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 112 °C
234 °F
ASTM D648
Flammability, UL94 HB
HB
Processing Properties Metric English Comments
Processing Temperature 210 - 250 °C
410 - 482 °F
Mold Temperature 60.0 - 80.0 °C
140 - 176 °F