Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ELASTO UK Dryflex® 5014-101 TPE, Modified Injection Molding Grade for General Applications

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer ELASTO UK Ltd, a Hexpol company
Trade Name Dryflex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ELASTO UK Dryflex® 5014-101 TPE, Modified Injection Molding Grade for General Applications.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The VTC TPE Group have developed endless formulations to fulfill different properties and application requirements to optimize the finished component. VTC Dryflex® 5014-101 is specifically designed for general use.Information from Vita Thermoplastic Polymers (VTP).Vita Thermoplastic Polymers was aquired by HEXPOL and is now ELASTO
Physical Properties Metric English Comments
Specific Gravity 1.01 g/cc
1.01 g/cc
ISO 2781
Melt Flow 1.7 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.7 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore A 50
50
ISO 868
Tensile Strength at Break 3.00 MPa
435 psi
ISO 37
Elongation at Break 560 %
560 %
ISO 37
100% Modulus 0.00170 GPa
0.247 ksi
ISO 37
Descriptive Properties Value Comments
Color Black