ELASTO UK Dryflex® 5029-104 TPE, Modified Injection Molding Grade for Door Stops

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer ELASTO UK Ltd, a Hexpol company
Trade Name Dryflex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ELASTO UK Dryflex® 5029-104 TPE, Modified Injection Molding Grade for Door Stops.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The VTC TPE Group have developed endless formulations to fulfill different properties and application requirements to optimize the finished component. VTC Dryflex® 5029-104 is specifically designed for door stops.Information from Vita Thermoplastic Polymers (VTP).Vita Thermoplastic Polymers was aquired by HEXPOL and is now ELASTO
Physical Properties Metric English Comments
Specific Gravity 1.45 g/cc
1.45 g/cc
ISO 2781
Melt Flow 7.5 g/10 min

@Load 5.00 kg,
Temperature 190 °C
7.5 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore A 62
62
ISO 868
Tensile Strength at Break 2.00 MPa
290 psi
ISO 37
Elongation at Break 450 %
450 %
ISO 37
100% Modulus 0.00130 GPa
0.189 ksi
ISO 37
Tear Strength 15.0 kN/m
85.6 pli
Method C; ISO 34
Descriptive Properties Value Comments
Color Black