Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

EMS-Grivory Grivory® AZ 3/2 PA66

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer EMS-Grivory (EMS-CHEMIE)
Trade Name Grivory®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Grivory Grivory® AZ 3/2 PA66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product description: Grilon AZ 3/2 is an unreinforced and impact modified PA66 injection molding grade. Grilon AZ 3/2 has the following important properties: Excellent toughness at low temperaturesExcellent toughness dry after molding Low density Grilon AZ 3/2 is a medium viscosity PA 66. Extrusion applications are possible, but Grilon AZ 3/2 is not recommended for extrusion applications, especially for extrudates which have a wall thickness less than 0.8 mm.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
ISO 1183
Water Absorption 8.0 %
8.0 %
ISO 62
Moisture Absorption 2.00 %
2.00 %
ISO 62
Linear Mold Shrinkage, Flow 0.016 cm/cm
0.016 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.018 cm/cm
0.018 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Ball Indentation Hardness 55.0 MPa
7980 psi
conditioned; ISO 2039-1
95.0 MPa
13800 psi
dry; ISO 2039-1
Tensile Stress 35.0 MPa

@Strain 50.0 %
5080 psi

@Strain 50.0 %
conditioned; ISO 527-1/-2
Tensile Strength, Yield 45.0 MPa
6530 psi
dry; ISO 527-1/-2
45.0 MPa
6530 psi
dry; ISO 527-1/-2
Elongation at Break >= 50 %
>= 50 %
dry; ISO 527-1/-2
>= 50 %
>= 50 %
conditioned; ISO 527-1/-2
<= 50 %
<= 50 %
dry; ISO 527-1/-2
Elongation at Yield 5.0 %
5.0 %
dry; ISO 527-1/-2
5.0 %
5.0 %
dry; ISO 527-1/-2
Tensile Modulus 0.700 GPa
102 ksi
conditioned; ISO 527-1/-2
1.70 GPa
247 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched NB
NB
dry; ISO 179/1eU
NB
NB
conditioned; ISO 179/1eU
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
dry; ISO 179/1eU
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched 9.00 J/cm²
42.8 ft-lb/in²
dry; ISO 179/1eA
NB
NB
conditioned; ISO 179/1eA
2.00 J/cm²

@Temperature 30.0 °C
9.52 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
2.00 J/cm²

@Temperature 30.0 °C
9.52 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 150 µm/m-°C
83.3 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 150 µm/m-°C
83.3 µin/in-°F
ISO 11359-1/-2
Melting Point 260 °C
500 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 90.0 - 110 °C
194 - 230 °F
long term; EMS
220 °C
428 °F
short term; EMS
Deflection Temperature at 0.46 MPa (66 psi) 170 °C
338 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C
149 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
conditioned; IEC 60093
1.00e+14 ohm-cm
1.00e+14 ohm-cm
dry; IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Strength 27.0 kV/mm
686 kV/in
conditioned; IEC 60243-1
29.0 kV/mm
737 kV/in
dry; IEC 60243-1
Comparative Tracking Index 600 V
600 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Automotive Powertrain and Chassis
Electricals & Electronics Connectors
Electrical appliances
Form Granules
Industry & Consumer goods Housewares
Mechanical Engineering
Sports & Leisure
Tools & Accessories
Processing Injection Molding
Product Attributes Improved friction & wear properties
Special Characteristics Flame retardant
High impact or impact modified
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved