EMS-Grivory Grivory® TSG-30/4 V0 PA666-GF30 FR

Category Polymer , Thermoplastic , Nylon , Nylon 6/66 , Nylon 66/6, 30% Glass Fiber Reinforced
Manufacturer EMS-Grivory (EMS-CHEMIE)
Trade Name Grivory®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Grivory Grivory® TSG-30/4 V0 PA666-GF30 FR.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product description: Grilon TSG-30/4 V0 is a heat stabilized, flame retardant, self-extinguishing engineering thermoplastic, reinforced with glass-fiber 30% (by weight) based on a semi-crystalline Polyamide-66- Polyamide-6-alloy. Grilon TSG-30/4 V0 is halogen-free and free of red phosphorus. The unpigmented material is of light inherent color. Besides its advantageous flame behavior, Grilon TSG-30/4 V0 exhibits high toughness and generally good mechanical properties.RoHS: Grilon TSG-30/4 V0 complies with the regulations acc. RoHS (2002/95/EC, Restriction of Hazardous Substances).WEEE: Parts made of Grilon TSG-30/4 V0 are not affected by the demands for "selective recycling" acc. guideline 2002/96/EC for Electro and Electronic Appliances Grilon TSG-30/4 V0 is particularly suited for technical injection molded parts in the field of Electro and Electronics which require a flammability rating of V-0 acc. UL 94.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.44 g/cc
0.0520 lb/in³
ISO 1183
Water Absorption 4.0 %
4.0 %
ISO 62
Moisture Absorption 1.50 %
1.50 %
ISO 62
Linear Mold Shrinkage, Flow 0.0020 cm/cm
0.0020 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0070 cm/cm
0.0070 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Ball Indentation Hardness 130 MPa
18900 psi
conditioned; ISO 2039-1
255 MPa
37000 psi
dry; ISO 2039-1
Tensile Strength at Break 90.0 MPa
13100 psi
conditioned; ISO 527-1/-2
150 MPa
21800 psi
dry; ISO 527-1/-2
Elongation at Break 2.5 %
2.5 %
dry; ISO 527-1/-2
4.5 %
4.5 %
conditioned; ISO 527-1/-2
Tensile Modulus 6.50 GPa
943 ksi
conditioned; ISO 527-1/-2
10.5 GPa
1520 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched 6.50 J/cm²
30.9 ft-lb/in²
dry; ISO 179/1eU
7.00 J/cm²
33.3 ft-lb/in²
conditioned; ISO 179/1eU
6.00 J/cm²

@Temperature 30.0 °C
28.6 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
6.00 J/cm²

@Temperature 30.0 °C
28.6 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched 0.950 J/cm²
4.52 ft-lb/in²
dry; ISO 179/1eA
1.40 J/cm²
6.66 ft-lb/in²
conditioned; ISO 179/1eA
0.850 J/cm²

@Temperature 30.0 °C
4.04 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
0.900 J/cm²

@Temperature 30.0 °C
4.28 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 100 - 120 °C
212 - 248 °F
long term; EMS
220 °C
428 °F
short term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 235 °C
455 °F
ISO 75-1/-2
Deflection Temperature at 8.0 MPa 165 °C
329 °F
ISO 75-1/-2
Flammability, UL94 V-0
V-0
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
dry; IEC 60093
1.00e+12 ohm-cm
1.00e+12 ohm-cm
conditioned; IEC 60093
Surface Resistance 1.00e+10 ohm
1.00e+10 ohm
IEC 60093
Comparative Tracking Index 600 V
600 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Automotive Automotive electr. and electronics, lighting
Burning Behaviour VDE
Electricals & Electronics Cables & Tubes
Connectors
Electrical appliances
Electrical equipment
Energy distribution
Lighting
Form Granules
Processing Injection Molding
Special Characteristics Flame retardant
Improved UV resistance (outdoor use)