Material Notes:
Product description: Grilon TSG-50/4 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 50% glass fibers. Grilon TSG-50/4 has the following important properties: High stiffnessGood flow behaviorGood surface finishEasy processing Application examples are stressed functional parts for automotive applications such as rear-view mirror brackets.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.55 g/cc
0.0560 lb/in³
ISO 1183
Water Absorption 5.0 %
5.0 %
ISO 62
Moisture Absorption 1.50 %
1.50 %
ISO 62
Linear Mold Shrinkage, Flow 0.0010 cm/cm
0.0010 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0030 cm/cm
0.0030 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Ball Indentation Hardness 160 MPa
23200 psi
conditioned; ISO 2039-1
280 MPa
40600 psi
dry; ISO 2039-1
Tensile Strength at Break 170 MPa
24700 psi
conditioned; ISO 527-1/-2
250 MPa
36300 psi
dry; ISO 527-1/-2
Elongation at Break 2.5 %
2.5 %
dry; ISO 527-1/-2
4.5 %
4.5 %
conditioned; ISO 527-1/-2
Tensile Modulus 12.5 GPa
1810 ksi
conditioned; ISO 527-1/-2
17.5 GPa
2540 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched 8.00 J/cm²
38.1 ft-lb/in²
dry; ISO 179/1eU
8.50 J/cm²
40.4 ft-lb/in²
conditioned; ISO 179/1eU
7.00 J/cm²

@Temperature 30.0 °C
33.3 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
8.00 J/cm²

@Temperature 30.0 °C
38.1 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched 1.40 J/cm²
6.66 ft-lb/in²
dry; ISO 179/1eA
2.00 J/cm²
9.52 ft-lb/in²
conditioned; ISO 179/1eA
1.20 J/cm²

@Temperature 30.0 °C
5.71 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
1.20 J/cm²

@Temperature 30.0 °C
5.71 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 15.0 µm/m-°C
8.33 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 90.0 µm/m-°C
50.0 µin/in-°F
ISO 11359-1/-2
Melting Point 260 °C
500 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 90.0 - 120 °C
194 - 248 °F
long term; EMS
200 °C
392 °F
short term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 250 °C
482 °F
ISO 75-1/-2
Deflection Temperature at 8.0 MPa 200 °C
392 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
conditioned; IEC 60093
1.00e+14 ohm-cm
1.00e+14 ohm-cm
dry; IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Strength 22.0 kV/mm
559 kV/in
conditioned; IEC 60243-1
27.0 kV/mm
686 kV/in
dry; IEC 60243-1
Comparative Tracking Index 550 V
550 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Automotive Air intake sytems
Powertrain and Chassis
Electricals & Electronics Electrical appliances
Electrical equipment
Form Granules
Industry & Consumer goods Housewares
Mechanical Engineering
Sports & Leisure
Tools & Accessories
Processing Injection Molding