Material Notes:
Product description: Grilamid XE 3959 natural is a high viscosity Polyamide 610 especially suitable for extrusion applications. This PA610 product is to a large extent based on renewable raw materials and its eco-profile is very favourable when compared to similar products based on crude oil. The main features of Grilamid XE 3959 natural are: Low volume expansion of tubes under pressureGood cold impact behaviourHigh heat and chemical resistanceEasy processing Grilamid XE 3959 natural can be processed on standard tube-extrusion lines suitable for polyamides. Grilamid XE 3959 natural was specially developed for automotive tubing applications for which a high long term usage and peak temperature are required. Grilamid XE 3959 natural has an excellent volume expansion behaviour and is particularly suitable for hydraulic clutch tubes.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
ISO 1183
Water Absorption 3.3 %
3.3 %
ISO 62
Moisture Absorption 1.60 %
1.60 %
ISO 62
Linear Mold Shrinkage, Flow 0.0090 cm/cm
0.0090 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0090 cm/cm
0.0090 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Ball Indentation Hardness 70.0 MPa
10200 psi
conditioned; ISO 2039-1
120 MPa
17400 psi
dry; ISO 2039-1
Tensile Strength at Break 40.0 MPa
5800 psi
dry; ISO 527-1/-2
60.0 MPa
8700 psi
conditioned; ISO 527-1/-2
Tensile Strength, Yield 45.0 MPa
6530 psi
dry; ISO 527-1/-2
60.0 MPa
8700 psi
dry; ISO 527-1/-2
Elongation at Break >= 50 %
>= 50 %
dry; ISO 527-1/-2
>= 50 %
>= 50 %
conditioned; ISO 527-1/-2
Elongation at Yield 5.0 %
5.0 %
dry; ISO 527-1/-2
18 %
18 %
conditioned; ISO 527-1/-2
Tensile Modulus 1.20 GPa
174 ksi
conditioned; ISO 527-1/-2
2.20 GPa
319 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched NB
NB
dry; ISO 179/1eU
NB
NB
conditioned; ISO 179/1eU
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
dry; ISO 179/1eU
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched 0.800 J/cm²
3.81 ft-lb/in²
dry; ISO 179/1eA
1.80 J/cm²
8.57 ft-lb/in²
conditioned; ISO 179/1eA
0.800 J/cm²

@Temperature 30.0 °C
3.81 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
0.900 J/cm²

@Temperature 30.0 °C
4.28 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 110 µm/m-°C
61.1 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 110 µm/m-°C
61.1 µin/in-°F
ISO 11359-1/-2
Melting Point 220 °C
428 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 110 - 130 °C
230 - 266 °F
long term; EMS
160 °C
320 °F
short term; EMS
Deflection Temperature at 0.46 MPa (66 psi) 150 °C
302 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C
131 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
dry; IEC 60093
1.00e+11 ohm-cm
1.00e+11 ohm-cm
conditioned; IEC 60093
Surface Resistance 1.00e+11 ohm
1.00e+11 ohm
IEC 60093
Dielectric Strength 34.0 kV/mm
864 kV/in
dry; IEC 60243-1
34.0 kV/mm
864 kV/in
conditioned; IEC 60243-1
Comparative Tracking Index 600 V
600 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Automotive Air intake sytems
Compressed air systems
Fuel systems
Hydraulic systems
Powertrain and Chassis
Electricals & Electronics Cables & Tubes
Form Granules
Industry & Consumer goods Hydraulics & Pneumatics
Mechanical Engineering
Tools & Accessories
Processing Other Extrusion
Profile Extrusion
Product Attributes Bio based Polyamide
High viscosity
Special Characteristics High impact or impact modified
Improved heat resistance
Improved UV resistance (outdoor use)
Light stabilized or stable to light
Copyright © lookpolymers.com All Rights Reserved