EMS-Grivory Grivory® XE 4105 nat PA610-GF50

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Nylon , Nylon 610 , Nylon 610, Glass Reinforced
Manufacturer EMS-Grivory (EMS-CHEMIE)
Trade Name Grivory®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Grivory Grivory® XE 4105 nat PA610-GF50.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product description: Grilamid XE 4105 natural is a 50% glass fiber reinforced, heat stabilized polyamide 610 (PA610) injection molding grade. This product is to a large extent based on renewable raw materials and its eco-profile is very favorable when compared to similar products based on crude oil. The main features of Grilamid XE 4105 are: High stiffnessLow water absorptionGood heat and chemical resistanceEasy processing Grilamid XE 4105 natural is particularly suitable for the manufacturing of technical injection molded parts in the application fields of: AutomotiveElectrical & Electronic goodsMechanical engineeringSports & leisure goodsDomestic appliancesInformation provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.53 g/cc
0.0553 lb/in³
ISO 1183
Water Absorption 1.9 %
1.9 %
ISO 62
Moisture Absorption 0.800 %
0.800 %
ISO 62
Linear Mold Shrinkage, Flow 0.0010 cm/cm
0.0010 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0070 cm/cm
0.0070 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Ball Indentation Hardness 165 MPa
23900 psi
conditioned; ISO 2039-1
225 MPa
32600 psi
dry; ISO 2039-1
Tensile Strength at Break 165 MPa
23900 psi
conditioned; ISO 527-1/-2
210 MPa
30500 psi
dry; ISO 527-1/-2
Elongation at Break 4.0 %
4.0 %
dry; ISO 527-1/-2
5.5 %
5.5 %
conditioned; ISO 527-1/-2
Tensile Modulus 12.0 GPa
1740 ksi
conditioned; ISO 527-1/-2
15.5 GPa
2250 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched 9.00 J/cm²
42.8 ft-lb/in²
conditioned; ISO 179/1eU
9.50 J/cm²
45.2 ft-lb/in²
dry; ISO 179/1eU
9.00 J/cm²

@Temperature 30.0 °C
42.8 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
9.50 J/cm²

@Temperature 30.0 °C
45.2 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
Charpy Impact, Notched 1.70 J/cm²
8.09 ft-lb/in²
dry; ISO 179/1eA
2.00 J/cm²
9.52 ft-lb/in²
conditioned; ISO 179/1eA
1.40 J/cm²

@Temperature 30.0 °C
6.66 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
1.40 J/cm²

@Temperature 30.0 °C
6.66 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 20.0 µm/m-°C
11.1 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 80.0 µm/m-°C
44.4 µin/in-°F
ISO 11359-1/-2
Melting Point 225 °C
437 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 100 - 130 °C
212 - 266 °F
long term; EMS
160 °C
320 °F
short term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 200 °C
392 °F
ISO 75-1/-2
Deflection Temperature at 8.0 MPa 150 °C
302 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
dry; IEC 60093
1.00e+12 ohm-cm
1.00e+12 ohm-cm
conditioned; IEC 60093
Surface Resistance 1.00e+11 ohm
1.00e+11 ohm
IEC 60093
Dielectric Strength 41.0 kV/mm
1040 kV/in
conditioned; IEC 60243-1
42.0 kV/mm
1070 kV/in
dry; IEC 60243-1
Comparative Tracking Index 600 V
600 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Automotive Air intake sytems
Automotive electr. and electronics, lighting
Compressed air systems
Cooling and climate control
Exterior
Fuel systems
Hydraulic systems
Interior
Powertrain and Chassis
Electricals & Electronics Connectors
Electrical appliances
Electrical equipment
Lighting
Mobile phones and other portable devices
Form Granules
Industry & Consumer goods Housewares
Hydraulics & Pneumatics
Mechanical Engineering
Power transmission
Sports & Leisure
Tools & Accessories
Processing Injection Molding
Product Attributes Bio based Polyamide
Special Characteristics Improved heat resistance
Improved UV resistance (outdoor use)
Light stabilized or stable to light
Copyright © lookpolymers.com All Rights Reserved