EMS-Grivory Grivory® XE 4176 black 9288 PA1010-GF50

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Nylon
Manufacturer EMS-Grivory (EMS-CHEMIE)
Trade Name Grivory®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Grivory Grivory® XE 4176 black 9288 PA1010-GF50.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product description: Grilamid XE 4176 black 9288 is a 50% glass fiber reinforced, heat stabilized polyamide 1010 injection molding grade. The main features of Grilamid XE 4176 black 9288 are: PA1010 Polymer fully based on renewable raw materialsvery low water absorptiongood chemical and UV resistancegood toughnesseasy processing Grilamid XE 4176 black 9288 is particularly suitable for the manufacturing of technical injection molded parts in the application fields of: AutomotiveElectrical & Electronic goodsMechanical engineeringSports & leisure goodsDomestic appliancesInformation provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.50 g/cc
0.0542 lb/in³
ISO 1183
Water Absorption 1.0 %
1.0 %
ISO 62
Moisture Absorption 0.500 %
0.500 %
ISO 62
Linear Mold Shrinkage, Flow 0.0010 cm/cm
0.0010 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0080 cm/cm
0.0080 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Ball Indentation Hardness 185 MPa
26800 psi
conditioned; ISO 2039-1
210 MPa
30500 psi
dry; ISO 2039-1
Tensile Strength at Break 150 MPa
21800 psi
conditioned; ISO 527-1/-2
170 MPa
24700 psi
dry; ISO 527-1/-2
Elongation at Break 4.0 %
4.0 %
dry; ISO 527-1/-2
4.5 %
4.5 %
conditioned; ISO 527-1/-2
Tensile Modulus 12.2 GPa
1770 ksi
conditioned; ISO 527-1/-2
14.0 GPa
2030 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched 9.00 J/cm²
42.8 ft-lb/in²
dry; ISO 179/1eU
9.00 J/cm²
42.8 ft-lb/in²
conditioned; ISO 179/1eU
9.00 J/cm²

@Temperature 30.0 °C
42.8 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
9.00 J/cm²

@Temperature 30.0 °C
42.8 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched 1.60 J/cm²
7.61 ft-lb/in²
dry; ISO 179/1eA
1.60 J/cm²
7.61 ft-lb/in²
conditioned; ISO 179/1eA
1.20 J/cm²

@Temperature 30.0 °C
5.71 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
1.20 J/cm²

@Temperature 30.0 °C
5.71 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 20.0 µm/m-°C
11.1 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 110 µm/m-°C
61.1 µin/in-°F
ISO 11359-1/-2
Melting Point 200 °C
392 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 180 °C
356 °F
ISO 75-1/-2
Deflection Temperature at 8.0 MPa 135 °C
275 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
dry; IEC 60093
1.00e+11 ohm-cm
1.00e+11 ohm-cm
conditioned; IEC 60093
Surface Resistance 1.00e+10 ohm
1.00e+10 ohm
IEC 60093
Dielectric Strength 35.0 kV/mm
889 kV/in
conditioned; IEC 60243-1
38.0 kV/mm
965 kV/in
dry; IEC 60243-1
Comparative Tracking Index 600 V
600 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Automotive Automotive electr. and electronics, lighting
Compressed air systems
Exterior
Fuel systems
Hydraulic systems
Interior
Powertrain and Chassis
Electricals & Electronics Connectors
Electrical appliances
Electrical equipment
Lighting
Form Granules
Industry & Consumer goods Housewares
Hydraulics & Pneumatics
Mechanical Engineering
Medical devices
Power transmission
Sports & Leisure
Tools & Accessories
Processing Injection Molding
Product Attributes Bio based Polyamide
Special Characteristics High impact or impact modified
Improved heat resistance
Improved UV resistance (outdoor use)
Light stabilized or stable to light