Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
ASTM D792, ISO 1183
Water Absorption 0.30 %

@Temperature 23.0 °C
0.30 %

@Temperature 73.4 °F
24h; ASTM D570, ISO 62
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
ASTM D955
Melt Index of Compound 15 - 20 g/10 min

@Load 10.0 kg,
Temperature 220 °C
15 - 20 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238, ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell L 105
105
ASTM D785, ISO 2039/2
Tensile Strength, Yield 45.0 MPa
6530 psi
ASTM D638, ISO R527
Elongation at Break >= 25 %
>= 25 %
ASTM D638, ISO R527
Flexural Modulus 2.40 GPa
348 ksi
ASTM D790, ISO 178
Izod Impact, Notched >= 1.20 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
>= 2.25 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256, ISO 180/4a
Thermal Properties Metric English Comments
Vicat Softening Point >= 95.0 °C

@Load 5.00 kg
>= 203 °F

@Load 11.0 lb
120°C/min; ASTM D1525/B, ISO 306/B
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
HB

@Thickness 3.20 mm
HB

@Thickness 0.126 in
Glow Wire Test 650 °C

@Thickness 3.20 mm
1200 °F

@Thickness 0.126 in
VDE 0471/P2-4, IEC 695
650 °C

@Thickness 2.00 mm
1200 °F

@Thickness 0.0787 in
VDE 0471/P2-4, IEC 695
Electrical Properties Metric English Comments
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
ASTM D257, IEC 93