Material Notes:
Extrusion grade; no additives. 811E as supplied by Eastman Chemical may lawfully be used in food contact (noncooking) subject to FDA 21 CFR 177.1520(c)(2.1).Information from manufacturer data sheet.Eastman Chemical Company sold its polyethylene business to Westlake Chemical Corporation in Dec. 2006. This grade no longer appears in the Westlake product line.
Physical Properties Metric English Comments
Density 0.916 g/cc
0.0331 lb/in³
ASTM D4883
Melt Flow 20 g/10 min

@Load 2.16 kg,
Temperature 190 °C
20 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 9.00 MPa
1310 psi
500 mm/min (20 in./min.); ASTM D638, Type IV Specimen
Tensile Strength, Yield 9.00 MPa
1310 psi
500 mm/min (20 in./min.); ASTM D638, Type IV Specimen
Elongation at Break 300 %
300 %
500 mm/min (20 in./min.); ASTM D638, Type IV Specimen
Flexural Modulus 0.172 GPa
24.9 ksi
2% Secant, 12.7 mm/min. (0.5 in./min.); ASTM D790
Thermal Properties Metric English Comments
Vicat Softening Point 85.0 °C
185 °F
ASTM D1525
Brittleness Temperature -45.0 °C
-49.0 °F
ASTM D746
Descriptive Properties Value Comments
Process Extrusion