Material Notes:
Voridian Aqua thermoplastic polyesters are condensation polymers produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. Voridian Aqua polymer 20837 was developed for the European sparkling water market and is available in Europe only.Applications/UsesWater bottles
Physical Properties Metric English Comments
Bulk Density 0.804 g/cc
0.0290 lb/in³
Poured; ASTM D1895
0.881 g/cc
0.0318 lb/in³
Vibrated; ASTM D1895
Density 1.40 g/cc
0.0506 lb/in³
Crystalline Density; ASTM D1505
Melt Density 1.20 g/cc

@Temperature 285 °C
0.0434 lb/in³

@Temperature 545 °F
ASTM D1238
Particle Size 2500 µm
2500 µm
Pellet Size
Viscosity Measurement 0.74 - 0.78
0.74 - 0.78
Intrinsic; VGAS-A-AN-G-V-1
Thermal Properties Metric English Comments
Heat of Fusion 61.0 J/g
26.2 BTU/lb
ASTM E793
Specific Heat Capacity 1.10 J/g-°C
0.263 BTU/lb-°F
ASTM E1269
1.40 J/g-°C

@Temperature 80.0 °C
0.335 BTU/lb-°F

@Temperature 176 °F
ASTM E1269
1.50 J/g-°C

@Temperature 100 °C
0.359 BTU/lb-°F

@Temperature 212 °F
ASTM E1269
1.90 J/g-°C

@Temperature 200 °C
0.454 BTU/lb-°F

@Temperature 392 °F
ASTM E1269
2.10 J/g-°C

@Temperature 280 °C
0.502 BTU/lb-°F

@Temperature 536 °F
ASTM E1269
Melting Point 248 °C
478 °F
Crystalline Peak Melting Point; ASTM D3418
Descriptive Properties Value Comments
Acetaldehyde <1ppm
VKCA-A-AS-G-GC-0001
Color, CIE a* -3.63 to -0.63
VGAS-A-AN-G-RS-001
Color, CIE b* -1.33 to 2.12
VGAS-A-AN-G-RS-001
Color, CIE L* 81 min
VGAS-A-AN-G-RS-001
Fines, wt%, max 0.05
Pellet Shape Cubical