Eastman Aqua PJ003 PET

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), Unreinforced
Manufacturer Eastman Chemical
Trade Name Aqua
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eastman Aqua PJ003 PET.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Voridian Aqua PET PJ003 is a condensation polymer produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. This product is specifically designed for large water container applications.Applications/UsesLarge water containersWater bottles
Physical Properties Metric English Comments
Bulk Density 0.800 g/cc
0.0289 lb/in³
Poured; ASTM D1895
0.870 g/cc
0.0314 lb/in³
Vibrated; ASTM D1895
Melt Density 1.20 g/cc

@Temperature 285 °C
0.0434 lb/in³

@Temperature 545 °F
ASTM D1238
Viscosity Measurement 0.78 - 0.82
0.78 - 0.82
Intrinsic; VGAS-A-AN-G-V-1
Thermal Properties Metric English Comments
Melting Point 240 °C
464 °F
Crystalline Peak Melting Point; ASTM D3418
Descriptive Properties Value Comments
Acetaldehyde <1ppm
VKCA-A-AS-G-GC-0001
Color, CIE L* 77.8 min
VGAS-A-AN-G-RS-001
Fines, wt%, max 0.1