Eastman CB12 PET  (discontinued **)

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), Unreinforced
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eastman CB12 PET  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Voridian CB12 polymer is a polyethylene terephthalate resin designed specifically for the carbonated soft drink (CSD) and other beverage markets. CB12 delivers fast, efficient processing and good overall bottle properties. This polymer is formulated to provide improved efficiencies in preform and bottle production while delivering a robust processing window. Bottles made with CB12 deliver improved barrier with continued excellent performance in creep and environmental stress-crack resistance.The pellets have a weight of 2.0g/100pelletsApplications/UsesBottlesCarbonated soft drink containersKey AttributesExcellent performance in stress-crack resistanceFast, efficient processingImproved barrierRobust processing window
Physical Properties Metric English Comments
Bulk Density 0.810 g/cc
0.0293 lb/in³
Poured (Mexico Produced); ASTM D1895
0.845 g/cc
0.0305 lb/in³
Poured (US Produced); ASTM D1895
0.880 g/cc
0.0318 lb/in³
Vibrated (Mexico Produced); ASTM D1895
0.898 g/cc
0.0324 lb/in³
Vibrated (US Produced); ASTM D1895
Density 1.40 g/cc
0.0506 lb/in³
Crystalline Density; ASTM D1505
Melt Density 1.20 g/cc

@Temperature 285 °C
0.0434 lb/in³

@Temperature 545 °F
ASTM D1238
Particle Size 2500 µm
2500 µm
Pellet Size
Viscosity Measurement 0.80 - 0.84
0.80 - 0.84
Intrinsic; EMN-A-AC-G-V-1
Thermal Properties Metric English Comments
Heat of Fusion 59.0 J/g
25.4 BTU/lb
ASTM E793
Specific Heat Capacity 1.20 J/g-°C
0.287 BTU/lb-°F
ASTM E1269
1.40 J/g-°C

@Temperature 80.0 °C
0.335 BTU/lb-°F

@Temperature 176 °F
ASTM E1269
1.50 J/g-°C

@Temperature 100 °C
0.359 BTU/lb-°F

@Temperature 212 °F
ASTM E1269
1.90 J/g-°C

@Temperature 200 °C
0.454 BTU/lb-°F

@Temperature 392 °F
ASTM E1269
2.10 J/g-°C

@Temperature 280 °C
0.502 BTU/lb-°F

@Temperature 536 °F
ASTM E1269
Melting Point 245 °C
473 °F
Crystalline Peak Melting Point; ASTM D3418
Descriptive Properties Value Comments
Acetaldehyde <3ppm
TEPO-A-AN-G-GC-67
Color, CIE a* -3.0 to 0.0
VGAS-A-AN-G-RS-001
Color, CIE b* -1.8 to 1.0
VGAS-A-AN-G-RS-001
Color, CIE L* 76.5 min
VGAS-A-AN-G-RS-001
Fines, wt%, max 0.05
VGAS-A-AN-G-GA-1
Pellet Shape Cubical
Copyright © lookpolymers.com All Rights Reserved