Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Eastman Cadence™ GS5 Clear (Unpigmented) Copolyester for film calendering

Category Polymer , Film , Thermoplastic , Polyester, TP , Polyester Film
Manufacturer Eastman Chemical
Trade Name Cadence™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eastman Cadence™ GS5 Clear (Unpigmented) Copolyester for film calendering.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Eastman Cadence™ copolyester, for calendered films, is a specialty plastic developed to meet the demand for an environmentally responsible material for the calendering industry. Available in different grades, it features ease of processing, high-melt strength, aesthetics, clarity and gloss.BenefitsCan be used on existing calendering lines with no or minimal modification.No drying is needed prior to the calendering process.Good thermal stability during normal calendering process conditions.No corrosive degradation products are normally formed.Easy to emboss for added texture and dimensions with standard engraved rolls. Easy to decorate using offset lithography, flexographic, and screen-printing processes.Thermoforms easily and is compatible with commercial adhesives used in lamination processesEnvironmentally responsible material.Product description: Eastman Cadence GS5 is an amorphous copolyester with improved processability for film calendering. Calendered films made of Eastman Cadence copolyesters are non-crystallizing, are halogen-free, offer wide calendering and thermoforming windows and have good low-temperature toughness. They are cooperative in secondary operations such as solvent-bonding, lamination, decoration, cold-forming, punching/cutting and embossment.Eastman Cadence resins require no pre-drying or additional stabilizers.Application/UsesAppliance filmsArchitectural laminatesAutomotive filmsBagsDecorative laminatesElectronic laminatesFloor coveringsFurniture/Furniture trimLabelsOutdoor filmsPackagingPrintable filmsShrink filmTransaction cardsTransportation laminatesWall coveringsReported typical properties are preliminary. Information was provided by Eastman.
Physical Properties Metric English Comments
Specific Gravity 1.27 g/cc
1.27 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 83
83
ASTM D2240
Hardness, Shore D 73
73
ASTM D2240
Secant Modulus, MD 1.87 GPa
271 ksi
Tangent; ASTM D882
Secant Modulus, TD 1.825 GPa
264.7 ksi
Tangent; ASTM D882
Film Tensile Strength at Break, MD 50.0 MPa
7250 psi
ASTM D882
Film Tensile Strength at Break, TD 48.0 MPa
6960 psi
ASTM D882
1% Secant Modulus, MD 1800 MPa
261000 psi
ASTM D882
1% Secant Modulus, TD 1760 MPa
255000 psi
ASTM D882
Thermal Properties Metric English Comments
Brittleness Temperature -45.0 °C
-49.0 °F
by Impact; ASTM D1790
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Descriptive Properties Value Comments
Greenguard Indoor Air Quality Certified yes