VORIDIAN low density polyethylene D4027-P is a formulation suggested for extrusion coating applications that require clarity, high gloss and superior hot tack properties. Applications/UsesFood PackagingEastman Chemical Company sold its polyethylene business to Westlake Chemical Corporation in Dec. 2006. This grade no longer appears in the Westlake product line.
Physical Properties Metric English Comments
Density 0.920 g/cc
0.0332 lb/in³
ASTM D4883
Melt Flow 1.7 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.7 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 12.0 MPa
1740 psi
500 mm/min; ASTM D638
Tensile Strength, Yield 10.0 MPa
1450 psi
500 mm/min; ASTM D638
Elongation at Break 500 %
500 %
500 mm/min; ASTM D638
Flexural Modulus 0.234 GPa
33.9 ksi
2% Secant, 12.7 mm/min; ASTM D790
Thermal Properties Metric English Comments
Vicat Softening Point 95.0 °C
203 °F
ASTM D1525
Brittleness Temperature <= -73.0 °C
<= -99.4 °F
ASTM D746