Material Notes:
Polyethylene E6838-889P is a formulation suggested for extrusion coating applications and has been used successfully in compounding. This product may be used for holding food during cooking.Applications/UsesFood packagingEastman Chemical Company sold its polyethylene business to Westlake Chemical Corporation in Dec. 2006. This grade no longer appears in the Westlake product line.
Physical Properties Metric English Comments
Density 0.917 g/cc
0.0331 lb/in³
ASTM D4883
Melt Flow 7.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
7.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 9.70 MPa
1410 psi
500 mm/min; ASTM D638
Tensile Strength, Yield 9.70 MPa
1410 psi
500 mm/min; ASTM D638
Elongation at Break 400 %
400 %
500 mm/min; ASTM D638
Flexural Modulus 0.172 GPa
24.9 ksi
2% Secant, 12.7 mm/min; ASTM D790
Thermal Properties Metric English Comments
Vicat Softening Point 86.0 °C
187 °F
ASTM D1525
Brittleness Temperature <= -73.0 °C
<= -99.4 °F
ASTM D746
Descriptive Properties Value Comments
Process Film