Material Notes:
Eastar AN001 Copolyester has excellent appearance and is nearly water-clear. Its most outstanding features are its chemical resistance and processing capabilities. Exposure to aromatic oils often causes crazing or actual fracture of many polymer resins, but AN001 maintains its physical properties when exposed to these oils, and its appearance is virtually unchanged.Applications/UsesCosmetics/personal care packagingFragrance packagingKey AttributesEffective barrier propertiesExcellent ClarityExcellent colorabilityGood stiffnessExcellent chemical resistanceToughnessEasy to extrude, cut, print, and sealHigh gloss appearanceGood impact strength
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Linear Mold Shrinkage 0.0020 - 0.0060 cm/cm

@Thickness 3.20 mm
0.0020 - 0.0060 in/in

@Thickness 0.126 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 103
103
ASTM D785
Tensile Strength at Break 51.0 MPa
7400 psi
ASTM D638
Tensile Strength, Yield 47.0 MPa
6820 psi
ASTM D638
Elongation at Break 320 %
320 %
ASTM D638
Elongation at Yield 5.0 %
5.0 %
ASTM D638
Flexural Yield Strength 69.0 MPa
10000 psi
ASTM D790
Flexural Modulus 2.00 GPa
290 ksi
ASTM D790
Izod Impact, Notched 0.400 J/cm

@Temperature -40.0 °C
0.749 ft-lb/in

@Temperature -40.0 °F
ASTM D256
0.800 J/cm

@Temperature 23.0 °C
1.50 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Izod Impact, Unnotched NB
NB
ASTM D4812
NB

@Temperature -40.0 °C
NB

@Temperature -40.0 °F
ASTM D4812
Puncture Energy 42.0 J
31.0 ft-lb
Puncture Resistance @Max Load, 23°C; ASTM D3763
48.0 J

@Temperature -40.0 °C
35.4 ft-lb

@Temperature -40.0 °F
Puncture Resistance at Max Load; ASTM D3763
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 73.0 °C
163 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C
149 °F
ASTM D648
Optical Properties Metric English Comments
Haze 0.30 %
0.30 %
ASTM D1003
Transmission, Visible 89 %
89 %
Regular Transmittance; ASTM D1003
91 %
91 %
Total Transmittance; ASTM D1003
Processing Properties Metric English Comments
Melt Temperature 230 - 280 °C
446 - 536 °F
Mold Temperature 15.0 - 30.0 °C
59.0 - 86.0 °F
Drying Temperature 70.0 °C
158 °F
Dry Time 3 hour
3 hour