Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Eastman Eastar GN046 Copolyester, Natural

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), Unreinforced
Manufacturer Eastman Chemical
Trade Name Eastar
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eastman Eastar GN046 Copolyester, Natural.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Eastar Copolyester GN046 is a very high melt strength copolyester targeted for extrusion blow molding applications. Blow molding of large parts (up to several pounds) are possible with this material. This product is certified to ANSI/NSF Standard 51.Applications/UsesBottlesKey AttributesEffective barrier propertiesExcellent ClarityExcellent colorabilityGood stiffnessExcellent chemical resistanceToughnessEasy to extrude, cut, print, and sealHigh gloss appearanceGood impact strength
Physical Properties Metric English Comments
Specific Gravity 1.27 g/cc
1.27 g/cc
ASTM D792
Linear Mold Shrinkage 0.0020 - 0.0050 cm/cm

@Thickness 3.20 mm
0.0020 - 0.0050 in/in

@Thickness 0.126 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 108
108
ASTM D785
Tensile Strength at Break 28.0 MPa
4060 psi
ASTM D638
Tensile Strength, Yield 50.0 MPa
7250 psi
ASTM D638
Elongation at Break 110 %
110 %
ASTM D638
Elongation at Yield 4.0 %
4.0 %
ASTM D638
Flexural Strength 68.0 MPa
9860 psi
ASTM D790
Flexural Modulus 2.10 GPa
305 ksi
ASTM D790
Izod Impact, Notched 0.530 J/cm

@Temperature -40.0 °C
0.993 ft-lb/in

@Temperature -40.0 °F
ASTM D256
0.940 J/cm

@Temperature 23.0 °C
1.76 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Izod Impact, Unnotched NB
NB
ASTM D4812
NB

@Temperature -40.0 °C
NB

@Temperature -40.0 °F
ASTM D4812
Puncture Energy 36.0 J
26.6 ft-lb
Puncture Resistance @Max Load, 23°C; ASTM D3763
35.0 J

@Temperature -40.0 °C
25.8 ft-lb

@Temperature -40.0 °F
Puncture Resistance at Max Load; ASTM D3763
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 70.0 °C
158 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 62.0 °C
144 °F
ASTM D648
Vicat Softening Point 83.0 °C
181 °F
1kg load; ASTM D1525
Optical Properties Metric English Comments
Haze 0.60 %
0.60 %
ASTM D1003
Gloss 152 %
152 %
at 60°; ASTM D2457
Transmission, Visible 87 %
87 %
Regular Transmittance; ASTM D1003
90 %
90 %
Total Transmittance; ASTM D1003
Processing Properties Metric English Comments
Melt Temperature 249 - 271 °C
480 - 520 °F
Mold Temperature 16.0 - 38.0 °C
60.8 - 100 °F
Drying Temperature 71.0 °C
160 °F
Dry Time 6 hour
6 hour