Eastman Eastar GN101 PETG Copolyester  (discontinued **)

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , PETG Copolyester
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eastman Eastar GN101 PETG Copolyester  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ISO data as provided by the manufacturer, Eastman Chemical
Physical Properties Metric English Comments
Density 1.27 g/cc
0.0459 lb/in³
Linear Mold Shrinkage, Flow 0.0020 - 0.0050 cm/cm
0.0020 - 0.0050 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Yield 51.0 MPa
7400 psi
50 mm/min
Elongation at Break >= 50 %
>= 50 %
Elongation at Yield 4.1 %
4.1 %
Tensile Modulus 2.03 GPa
294 ksi
1mm/min
Charpy Impact Unnotched NB
NB
NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
Charpy Impact, Notched 0.530 J/cm²
2.52 ft-lb/in²
0.310 J/cm²

@Temperature -30.0 °C
1.48 ft-lb/in²

@Temperature -22.0 °F
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 43.0 µm/m-°C

@Temperature 20.0 °C
23.9 µin/in-°F

@Temperature 68.0 °F
CTE, linear, Transverse to Flow 59.0 µm/m-°C

@Temperature 20.0 °C
32.8 µin/in-°F

@Temperature 68.0 °F
Specific Heat Capacity 1.30 J/g-°C
0.311 BTU/lb-°F
Thermal Conductivity 0.190 W/m-K
1.32 BTU-in/hr-ft²-°F
Deflection Temperature at 0.46 MPa (66 psi) 71.0 °C
160 °F
Deflection Temperature at 1.8 MPa (264 psi) 63.0 °C
145 °F
Vicat Softening Point 73.0 °C
163 °F
Glass Transition Temp, Tg 79.0 °C
174 °F
Processing Properties Metric English Comments
Melt Temperature 250 - 270 °C
482 - 518 °F