Material Notes:
M3016-P is suggested for applications such as spiral-wound can linings, release paper, and photographic paper. M3016-P Has been found to exhibit good barrier properties, temperature resistance, and stress crack resistance.Information supplied by the manufacturer.Information from manufacturer data sheet.Eastman Chemical Company sold its polyethylene business to Westlake Chemical Corporation in Dec. 2006. This grade no longer appears in the Westlake product line.
Physical Properties Metric English Comments
Density 0.946 g/cc
0.0342 lb/in³
ASTM D4883
Melt Flow 10 g/10 min

@Load 2.16 kg,
Temperature 190 °C
10 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 22.0 MPa
3190 psi
500 mm/min (20 in./min.); ASTM D638, Type IV Specimen
Tensile Strength, Yield 25.0 MPa
3630 psi
500 mm/min (20 in./min.); ASTM D638, Type IV Specimen
Elongation at Break 20 %
20 %
500 mm/min (20 in./min.); ASTM D638, Type IV Specimen
Flexural Modulus 0.896 GPa
130 ksi
2% Secant, 12.7 mm/min. (0.5 in./min.); ASTM D790
Thermal Properties Metric English Comments
Vicat Softening Point 114 °C
237 °F