Eastman Tenite 285A2R30020 Cellulose Acetate Butyrate, Natural, Trsp

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Cellulosic , Cellulose Acetate Butyrate, Molded
Manufacturer Eastman Chemical
Trade Name Tenite
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eastman Tenite 285A2R30020 Cellulose Acetate Butyrate, Natural, Trsp.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications:Tool handlesToys/sporting goodsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosic plastics differ with plasticizer levels. Lower plasticizer content yields a harder surface, higher heat resistance, greater rigidity, higher tensile strength, and better dimensional stability. Higher plasticizer content increases impact strength. Tenite cellulose plastics are available in natural, clear, selected ambers, or smoke transparents and black translucents. Color concentrates are available in let-down ratios from 10:1 to 40:1. Tenite Cellulose Acetate Butyrate 285-20 has a plasticizer level of 20% and contains an odor mask.Information provided by Eastman.
Physical Properties Metric English Comments
Specific Gravity 1.17 g/cc
1.17 g/cc
ASTM D792
Water Absorption 1.2 %

@Time 86400 sec
1.2 %

@Time 24.0 hour
Immersion; ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell R 12
12
ASTM D785
Tensile Strength at Break 27.6 MPa
4000 psi
ASTM D638
Tensile Strength, Yield 21.4 MPa
3100 psi
ASTM D638
Elongation at Break 50 %
50 %
ASTM D638
Flexural Strength 27.6 MPa
4000 psi
ASTM D790
Flexural Modulus 0.965 GPa
140 ksi
ASTM D790
Izod Impact, Notched 1.12 J/cm

@Temperature -40.0 °C
2.10 ft-lb/in

@Temperature -40.0 °F
ASTM D256
3.84 J/cm

@Temperature 23.0 °C
7.19 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 72.0 °C
162 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 58.0 °C
136 °F
ASTM D648
Vicat Softening Point 92.0 °C
198 °F
ASTM D1525
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Descriptive Properties Value Comments
Formula Number 285
Odor Mask
Plasticizer 20 percent
Soluble Matter Loss 0.1 percent
ASTM D570
Weight Loss on Heating 1 percent
ASTM D707, 72 hrs, 80°C