Eastman Tenite 572A1V95316 Cellulose Acetate Butyrate, Smoke, Trsp

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Cellulosic , Cellulose Acetate Butyrate, Molded
Manufacturer Eastman Chemical
Trade Name Tenite
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eastman Tenite 572A1V95316 Cellulose Acetate Butyrate, Smoke, Trsp.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications:Molded partsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosic plastics differ with plasticizer levels. Lower plasticizer content yields a harder surface, higher heat resistance, greater rigidity, higher tensile strength, and better dimensional stability. Higher plasticizer content increases impact strength. Tenite cellulosic plastics are available in natural, clear, selected ambers or smoke transparents and black translucents. Color concentrates are available in let-down ratios from 10:1 to 40:1. Tenite Cellulose Acetate Butyrate 572-16 contains an odor mask lubricant and an ultra-violet inhibitor (UVI). It has a plasticizer level of 16%.Information provided by Eastman.
Physical Properties Metric English Comments
Specific Gravity 1.19 g/cc
1.19 g/cc
ASTM D792
Water Absorption 1.2 %

@Time 86400 sec
1.2 %

@Time 24.0 hour
Immersion; ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell R 60
60
ASTM D785
Tensile Strength at Break 31.0 MPa
4500 psi
ASTM D638
Tensile Strength, Yield 30.3 MPa
4390 psi
ASTM D638
Elongation at Break 26 %
26 %
ASTM D638
Flexural Modulus 1.162 GPa
168.5 ksi
ASTM D790
Izod Impact, Notched 1.02 J/cm

@Temperature -40.0 °C
1.91 ft-lb/in

@Temperature -40.0 °F
ASTM D256
5.31 J/cm

@Temperature 23.0 °C
9.95 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 79.0 °C
174 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 67.0 °C
153 °F
ASTM D648
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Descriptive Properties Value Comments
Formula Number 572
UVI; odor mask
Plasticizer 16 percent
Weight Loss on Heating 0.9 percent
ASTM D707, 72 hrs, 80°C