Material Notes:
Eastman Tritan FX200 is an amorphous copolyester that combines clarity and toughness with heat and chemical resistance. Films manufactured from this new-generation copolyester can be thermoformed without pre-drying and with a wide processing window that allows for product designs that reflect intricate detail.Application/UsesConsumer and durable goodsGraphic artsLeisure and safetySpecialty filmsKey AttributesDoes not contain Bisphenol-A (BPA)Does not contain plasticizersExcellent clarityVery good heat resistanceNo pre-drying of film prior to thermoformingGood chemical resistanceGood toughnessWide thermoforming windowInformation was provided by Eastman.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ASTM D1505
Water Absorption 0.50 %

@Time 86400 sec
0.50 %

@Time 24.0 hour
ASTM D570
Water Vapor Transmission 4.00 g/m²/day

@Temperature 23.0 °C
0.258 g/100 in²/day

@Temperature 73.4 °F
ASTM F1249
10.0 g/m²/day

@Temperature 38.0 °C
0.644 g/100 in²/day

@Temperature 100 °F
ASTM F1249
Oxygen Transmission 44.0 cc-mm/m²-24hr-atm
112 cc-mil/100 in²-24hr-atm
ASTM D3985
Carbon Dioxide Transmission 211 cc-mm/m²-24hr-atm
536 cc-mil/100 in²-24hr-atm
ASTM D1434
Thickness 254 microns
10.0 mil
Thickness of film tested; ASTM D374
Surface Tension 8.0 dynes/cm
8.0 dynes/cm
Polar; ASTM D5946
39 dynes/cm
39 dynes/cm
Dispersive; ASTM D5946
47 dynes/cm
47 dynes/cm
Total; ASTM D5946
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 43.0 MPa
6240 psi
ASTM D882
Film Tensile Strength at Yield, TD 41.0 MPa
5950 psi
ASTM D882
Film Elongation at Break, MD 114 %
114 %
ASTM D882
Film Elongation at Break, TD 115 %
115 %
ASTM D882
Film Elongation at Yield, MD 8.0 %
8.0 %
ASTM D882
Film Elongation at Yield, TD 8.0 %
8.0 %
ASTM D882
Secant Modulus, MD 1.50 GPa
218 ksi
Tangent; ASTM D882
Secant Modulus, TD 1.40 GPa
203 ksi
Tangent; ASTM D882
Puncture Energy 4.50 J
3.32 ft-lb
Dynatup; ASTM D3763
Tear Strength 9.00 kN/m
51.4 pli
TD; Trouser @200/mm/min; ISO 6383-1
9.00 kN/m
51.4 pli
Split tear method, TD; ASTM D1938
10.0 kN/m
57.1 pli
MD; Trouser @200/mm/min; ISO 6383-1
10.0 kN/m
57.1 pli
Split tear method, MD; ASTM D1938
Elmendorf Tear Strength MD 377 g
377 g
ASTM D1922
Elmendorf Tear Strength TD 428 g
428 g
ASTM D1922
Elmendorf Tear Strength, MD 1.50 g/micron
38.1 g/mil
ASTM D1922
Elmendorf Tear Strength, TD 1.70 g/micron
43.2 g/mil
ASTM D1922
Dart Drop 3.20 g/micron

@Temperature 23.0 °C
81.3 g/mil

@Temperature 73.4 °F
ASTM 1709A
3.20 g/micron

@Temperature -18.0 °C
81.3 g/mil

@Temperature -0.400 °F
ASTM 1709A
3.20 g/micron

@Temperature -30.0 °C
81.3 g/mil

@Temperature -22.0 °F
ASTM 1709A
Dart Drop Test 825 g

@Temperature 23.0 °C
1.82 lb

@Temperature 73.4 °F
ASTM 1709A
825 g

@Temperature -18.0 °C
1.82 lb

@Temperature -0.400 °F
ASTM 1709A
852 g

@Temperature -30.0 °C
1.88 lb

@Temperature -22.0 °F
ASTM 1709A
Film Tensile Strength at Break, MD 57.0 MPa
8270 psi
ASTM D882
Film Tensile Strength at Break, TD 42.0 MPa
6090 psi
ASTM D882
Thermal Properties Metric English Comments
CTE, linear 80.0 µm/m-°C
44.4 µin/in-°F
ASTM D696
Specific Heat Capacity 1.76 J/g-°C

@Temperature 60.0 °C
0.420 BTU/lb-°F

@Temperature 140 °F
DSC
1.92 J/g-°C

@Temperature 100 °C
0.460 BTU/lb-°F

@Temperature 212 °F
DSC
2.26 J/g-°C

@Temperature 150 °C
0.540 BTU/lb-°F

@Temperature 302 °F
DSC
2.43 J/g-°C

@Temperature 200 °C
0.580 BTU/lb-°F

@Temperature 392 °F
DSC
2.59 J/g-°C

@Temperature 250 °C
0.620 BTU/lb-°F

@Temperature 482 °F
DSC
Glass Transition Temp, Tg 119 °C
246 °F
DSC
Optical Properties Metric English Comments
Refractive Index 1.54
1.54
ASTM D542
Haze 0.80 %
0.80 %
ASTM D1003
Gloss 158 %
158 %
@ 60°; ASTM D2457
Yellow Index 0.50 %
0.50 %
ASTM D1925
Transmission, Visible 93 %
93 %
ASTM D1003
UV Transmittance 89 %

@Thickness 0.380 mm
89 %

@Thickness 0.0150 in
UV/Vis Spectro
Compliance Properties Metric English Comments
FDA Yes
Yes
Repeated use food contact articles
NSF Yes
Yes
Food equipment materials; NSF/ANSI Standard 51
Descriptive Properties Value Comments
PPT Tear Resistance, M.D. 40 N
ASTM D2582
PPT Tear Resistance, T.D. 40 N
ASTM D2582
Taber Abrasion 20% haze
ASTM 1044, Average at 25 cycles