Material Notes:
Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsTungsten Powder Filled Co-Polyamide (COPA)Excellent ToughnessInformation provided by Technical Polymers
Physical Properties Metric English Comments
Specific Gravity 3.80 g/cc
3.80 g/cc
ASTM D792
Linear Mold Shrinkage 0.010 - 0.012 cm/cm
0.010 - 0.012 in/in
Internal
Mechanical Properties Metric English Comments
Tensile Strength at Break 29.0 MPa
4210 psi
ISO 527
Elongation at Break 76.4 %
76.4 %
ISO 527
Tensile Modulus 0.979 GPa
142 ksi
ISO 527
Flexural Modulus 0.870 GPa
126 ksi
ISO 178
Izod Impact, Notched (ISO) 6.80 kJ/m²
3.24 ft-lb/in²
ISO 180-A
Processing Properties Metric English Comments
Melt Temperature 230 - 250 °C
446 - 482 °F
Mold Temperature 65.0 - 80.0 °C
149 - 176 °F
Drying Temperature 75.0 °C
167 °F
Dry Time 4 hour
4 hour