Ecomass® 1080ZC86 Stainless Steel Powder Filled Polyamide Alloy, Injection Molding

Category Polymer , Thermoplastic , Nylon
Manufacturer Ecomass Technologies
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ecomass® 1080ZC86 Stainless Steel Powder Filled Polyamide Alloy, Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Stainless Steel Powder Filled Polyamide Alloy, Very Good Toughness, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, weighting, balancing and radiation shielding applicationsInformation provided by Technical Polymers.
Physical Properties Metric English Comments
Specific Gravity 4.00 g/cc
4.00 g/cc
Internal Method
Linear Mold Shrinkage 0.0080 - 0.010 cm/cm
0.0080 - 0.010 in/in
Mechanical Properties Metric English Comments
Tensile Strength 28.0 MPa
4060 psi
ISO 527
Elongation at Break 2.0 %
2.0 %
ISO 527
Tensile Modulus 7.00 GPa
1020 ksi
ISO 527
Flexural Modulus 6.00 GPa
870 ksi
ISO 178
Processing Properties Metric English Comments
Melt Temperature 230 - 250 °C
446 - 482 °F
Mold Temperature 65.0 - 80.0 °C
149 - 176 °F
Drying Temperature 80.0 °C
176 °F
Dry Time 4 - 6 hour
4 - 6 hour
Moisture Content <= 0.20 %
<= 0.20 %
target