Ecomass® 4301TU74 Tungsten Filled Polyphthalamide

Category Polymer , Thermoplastic , Polyphthalamide (PPA)
Manufacturer Ecomass Technologies
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ecomass® 4301TU74 Tungsten Filled Polyphthalamide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsTungsten Powder Filled Polyphthalamide (PPA)Very Good ToughnessInformation provided by Technical Polymers
Physical Properties Metric English Comments
Specific Gravity 3.80 g/cc
3.80 g/cc
ASTM D792
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
Internal
Mechanical Properties Metric English Comments
Tensile Strength at Break 82.0 MPa
11900 psi
ISO 527
Elongation at Break 3.6 %
3.6 %
ISO 527
Tensile Modulus 4.409 GPa
639.5 ksi
ISO 527
Flexural Modulus 4.169 GPa
604.7 ksi
ISO 178
Izod Impact, Notched (ISO) 6.00 kJ/m²
2.86 ft-lb/in²
ISO 180-A
Processing Properties Metric English Comments
Melt Temperature 310 - 330 °C
590 - 626 °F
Drying Temperature 80.0 °C
176 °F
Dry Time 4 - 8 hour
4 - 8 hour
Moisture Content <= 0.10 %
<= 0.10 %