Material Notes:
Elastocon® 2825 thermoplastic elastomer compound has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® 2825 is FDA compliant and well suited for consumer goods and industrial applications requiring non-slip/soft touch ergonomics and resilience. Elastocon® 2825 can be overmolded onto polypropylene.Information provided by Elastocon® TPE Technologies
Physical Properties Metric English Comments
Specific Gravity 0.880 g/cc
0.880 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.022 - 0.032 cm/cm
0.022 - 0.032 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore A 25
25
ASTM D2240
Tensile Strength, Yield 4.94 MPa
716 psi
ASTM D412
Elongation at Break 530 %
530 %
ASTM D412
100% Modulus 0.000724 GPa
0.105 ksi
ASTM D412
Compression Set 13 %

@Time 79200 sec
13 %

@Time 22.0 hour
ASTM D395B
Processing Properties Metric English Comments
Feed Temperature 79.4 °C
175 °F
Rear Barrel Temperature 138 - 160 °C
280 - 320 °F
Front Barrel Temperature 166 - 182 °C
330 - 360 °F
Nozzle Temperature 188 - 204 °C
370 - 400 °F
Mold Temperature 15.6 - 48.9 °C
60.0 - 120 °F
Back Pressure 0.345 - 0.689 MPa
50.0 - 100 psi
Descriptive Properties Value Comments
Injection Rate Fast