Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Elastomer Engineering Elastamide 400 Elastomer Modified RIM Nylon 6

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Impact Grade
Manufacturer Elastomer Engineering
Trade Name Elastamide
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Elastomer Engineering Elastamide 400 Elastomer Modified RIM Nylon 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
18% crystallinity. Information supplied by Elastomer Engineering.
Physical Properties Metric English Comments
Water Absorption 1.6 %
1.6 %
24 hrs; DIN 53714
Mechanical Properties Metric English Comments
Hardness, Shore D 52
52
Tensile Strength, Ultimate 22.0 MPa
3190 psi
ASTM D638
Elongation at Break 420 %
420 %
ASTM D638
Tensile Modulus 0.230 GPa
33.4 ksi
ASTM D638
Flexural Modulus 0.240 GPa
34.8 ksi
ASTM D790
Taber Abrasion, mg/1000 Cycles 19
19
Electrical Properties Metric English Comments
Dielectric Constant 4.8

@Frequency 100000 Hz
4.8

@Frequency 100000 Hz
8.7

@Frequency 1000 Hz
8.7

@Frequency 1000 Hz
15.4

@Frequency 50 Hz
15.4

@Frequency 50 Hz
Dielectric Strength 14.0 kV/mm
356 kV/in
Dissipation Factor 0.10

@Frequency 100000 Hz
0.10

@Frequency 100000 Hz
ASTM D150
0.40

@Frequency 1000 Hz
0.40

@Frequency 1000 Hz
ASTM D150
Comparative Tracking Index 600 V
600 V
ASTM D257