Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Elastron® TPO Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Olefinic Elastomer (TPO)
Manufacturer Elastron
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Elastron® TPO Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
wide hardness rangedoes not require vulcanization-quite higher saving on the processing costsremains flexible at low temperatureshigh temperature resistanceelectrical insulator with very low conductivityhas grades with very low conductivitygrades with very high abrasion resistanceexcellent tear resistance100% recyclablePVC freeresistance to solventsresistance to oilresistance to acids, bases, and detergentsresistance to UV and ozoneresistance to bacterial and fungus growthhas low toxic potential, with many grades conforming with FDA regulationshalogen free flame retardancycoloured grades availableallows direct coloring during processing by utilizing colored PP and PE masterbatches2-shot molding onto many other plasticsappropriate co-extrusion process
Physical Properties Metric English Comments
Density >= 0.880 g/cc
>= 0.0318 lb/in³
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
Hardness, Shore D 65
65
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 100 °C
212 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Shrinkage 1.0 - 3.0 %
1.0 - 3.0 %
Processing Properties Metric English Comments
Rear Barrel Temperature 180 - 210 °C
356 - 410 °F
Middle Barrel Temperature 180 - 210 °C
356 - 410 °F
Front Barrel Temperature 180 - 210 °C
356 - 410 °F
Die Temperature 180 - 210 °C
356 - 410 °F
Mold Temperature 30.0 - 60.0 °C
86.0 - 140 °F
Descriptive Properties Value Comments
Acid-Base Resistance excellent
Comp. Ratio 2.5 - 3.5
Compression Set medium
Draw Down 5-10
Drying not necessary
Injection Speed medium-fast
L/D Ratio 20 - 24:1
Motor Oil Resistance medium
Solvent Resistance medium
UV-Ozone Stability very good
Users viewing this material also viewed the following: