Elektro-Isola Etronax DN Phenolic, Cotton Fabric Reinforcement, Brown, Tubes

Category Polymer , Thermoset , Phenolic
Manufacturer Elektro-Isola
Trade Name Etronax
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Elektro-Isola Etronax DN Phenolic, Cotton Fabric Reinforcement, Brown, Tubes.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: A strong and tough material. Very low water absorption and the lowest swelling in water. Very good low-friction material. High wear resistance in aggressive and dust-filled environments. Can be lubricated with water, oil or grease. Good dry-run properties.Applications: Bearing bushings and guide rings for hydraulic cylinders.Information provided by Elektro-Isola
Physical Properties Metric English Comments
Density 1.15 g/cc

@Thickness >=0.000 mm
0.0415 lb/in³

@Thickness >=0.000 in
24hr/23°C/50% RH; ISO 1183-A; IEC/EN 61212-2 7.3
Water Absorption 0.10 %
0.10 %
24hr/50°C+24hr in water at 23°C; ISO 62-1; IEC/EN 61212-2 7.2
Mechanical Properties Metric English Comments
Flexural Strength 85.0 MPa

@Diameter >=100 mm
12300 psi

@Diameter >=3.94 in
24hr/23°C/50% RH; ISO 178; IEC/EN 61212-2 5.1
Compressive Strength 140 MPa

@Temperature 23.0 °C,
Time 86400 sec
20300 psi

@Temperature 73.4 °F,
Time 24.0 hour
50% RH, Axial; ISO 604; IEC/EN 61212-2 5.2
Adhesive Bond Strength 180 MPa

@Diameter <=100 mm
26100 psi

@Diameter <=3.94 in
24hr/23°C/50% RH; IEC 60212-2; IEC/EN 61212-2 5.3
Thermal Properties Metric English Comments
Maximum Service Temperature, Inert 130 °C

@Thickness 3.00 mm,
Time 7.20e+7 sec
266 °F

@Thickness 0.118 in,
Time 20000 hour
IEC 60695-11-10; IEC/EN 61212-2 7.1
Electrical Properties Metric English Comments
Insulation Resistance 5.00e+9 ohm

@Diameter 8.00 - 10.0 mm
5.00e+9 ohm

@Diameter 0.315 - 0.394 in
24hr/50°C+24h in water at 23°C; IEC; IEC/EN 61212-2 6.2
Dielectric Constant 4.0

@Frequency 50.0 Hz
4.0

@Frequency 50.0 Hz
96hr/105°C+1hr/23°C/20%RH; IEC 250; IEC/EN 61212-2 6.3
Dielectric Strength 3.00 kV/mm

@Thickness 3.00 mm
76.2 kV/in

@Thickness 0.118 in
24hr/23°C/50% RH+1hr/oil 90°C; Perpendicular; IEC 60243-1; IEC/EN 61212-2 6.1.2.1
2.00 kV/mm

@Diameter >=3.00 mm
50.8 kV/in

@Diameter >=0.118 in
24hr/23°C/50% RH+1hr/oil 90°C; Parallel; IEC 60243-1; IEC/EN 61212-2 6.1.2.1
Dissipation Factor 0.040

@Frequency 50.0 Hz
0.040

@Frequency 50.0 Hz
96hr/105°C+1hr/23°C/20%RH; IEC 250; IEC/EN 61212-2 6.3