Description: Exclusively for mechanical applications. Impact-resistant, resistant to mechanical wear, noise-reducing, low friction. Well suited for parts where there are high mechanical load and wear. Good wear resistance in aggressive and dust-filled environments. Can be lubricated with water, oil or grease. Resistant to weather and salt water. Alternative to material containing asbestos.Information provided by Elektro-Isola
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
24hr/23°C/50% RH; ISO 1183-A; IEC/EN 60893-2 8.1
Water Absorption 1.6 %
1.6 %
24hr/50°C+24hr in water at 23°C,Test Specimen 50x50x3[mm]; ISO 62-1; IEC/EN 60893-2 8.2
Mechanical Properties Metric English Comments
Tensile Strength 80.0 MPa

@Thickness >=1.50 mm
11600 psi

@Thickness >=0.0591 in
24hr/23°C/50% RH; ISO 527; IEC/EN 60893-2 5.6
Modulus of Elasticity 7.00 GPa

@Thickness >=1.50 mm
1020 ksi

@Thickness >=0.0591 in
24hr/23°C/50% RH; ISO 178; IEC/EN 60893-2 5.2
Flexural Strength 115 MPa

@Thickness >=1.50 mm
16700 psi

@Thickness >=0.0591 in
24hr/23°C/50% RH; ISO 178; IEC/EN 60893-2 5.1
Compressive Strength 320 MPa

@Thickness >=5.00 mm
46400 psi

@Thickness >=0.197 in
24hr/23°C/50% RH; ISO 604; IEC/EN 60893-2 5.3
Shear Strength 40.0 MPa

@Thickness >=5.00 mm
5800 psi

@Thickness >=0.197 in
24hr/23°C/50% RH; IEC/EN 60893-2 5.5
Izod Impact, Notched (ISO) 10.0 kJ/m²

@Thickness >=5.00 mm
4.76 ft-lb/in²

@Thickness >=0.197 in
24hr/23°C/50% RH; ISO 180/2A; IEC/EN 60893-2 5.4.3
Thermal Properties Metric English Comments
Maximum Service Temperature, Inert 100 °C

@Thickness 0.000 mm,
Time 7.20e+7 sec
212 °F

@Thickness 0.000 in,
Time 20000 hour
IEC 60216; IEC/EN 60893-2 7.1
Electrical Properties Metric English Comments
Insulation Resistance 1.00e+6 ohm

@Thickness >=3.00 mm
1.00e+6 ohm

@Thickness >=0.118 in
24hr/50°C+24h in water at 23°C; IEC 60167; IEC/EN 60893-2 6.3
Dielectric Strength 0.200 kV/mm

@Thickness >=3.00 mm
5.08 kV/in

@Thickness >=0.118 in
24hr/23°C/50% RH+1hr/oil 90°C; Parallel; IEC 60245-1; IEC/EN 60893-2 6.1.3.2
1.00 kV/mm

@Thickness 3.00 mm
25.4 kV/in

@Thickness 0.118 in
24hr/23°C/50% RH+1hr/oil 90°C; Perpendicular; IEC 60245-1; IEC/EN 60893-2 6.1.3.1
Comparative Tracking Index 100 V

@Thickness 3.00 mm
100 V

@Thickness 0.118 in
IEC 60112; IEC/EN 60893-2 6.4