Material Notes:
Description: Reinforced with a finer cotton fabric than Etronax MF. Also well suited in particular for small components which are subject to mechanical load and wear. Can be machined to finer tolerances and smoother surface finish and Etronax MF.Information provided by Elektro-Isola
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
24hr/23°C/50% RH; ISO 1183-A; IEC/EN 60893-2 8.1
Water Absorption 1.33 %
1.33 %
24hr/50°C+24hr in water at 23°C,Test Specimen 50x50x3[mm]; ISO 62-1; IEC/EN 60893-2 8.2
Mechanical Properties Metric English Comments
Tensile Strength 100 MPa

@Thickness >=1.50 mm
14500 psi

@Thickness >=0.0591 in
24hr/23°C/50% RH; ISO 527; IEC/EN 60893-2 5.6
Modulus of Elasticity 7.00 GPa

@Thickness >=1.50 mm
1020 ksi

@Thickness >=0.0591 in
24hr/23°C/50% RH; ISO 178; IEC/EN 60893-2 5.2
Flexural Strength 130 MPa

@Thickness >=1.50 mm
18900 psi

@Thickness >=0.0591 in
24hr/23°C/50% RH; ISO 178; IEC/EN 60893-2 5.1
Compressive Strength 280 MPa

@Thickness >=5.00 mm
40600 psi

@Thickness >=0.197 in
24hr/23°C/50% RH; ISO 604; IEC/EN 60893-2 5.3
Shear Strength 50.0 MPa

@Thickness >=5.00 mm
7250 psi

@Thickness >=0.197 in
24hr/23°C/50% RH; IEC/EN 60893-2 5.5
Izod Impact, Notched (ISO) 7.00 kJ/m²

@Thickness >=5.00 mm
3.33 ft-lb/in²

@Thickness >=0.197 in
24hr/23°C/50% RH; ISO 180/2A; IEC/EN 60893-2 5.4.3
Thermal Properties Metric English Comments
Maximum Service Temperature, Inert 100 °C

@Thickness 0.000 mm,
Time 7.20e+7 sec
212 °F

@Thickness 0.000 in,
Time 20000 hour
IEC 60216; IEC/EN 60893-2 7.1
Electrical Properties Metric English Comments
Insulation Resistance 1.00e+6 ohm

@Thickness >=3.00 mm
1.00e+6 ohm

@Thickness >=0.118 in
24hr/50°C+24h in water at 23°C; IEC 60167; IEC/EN 60893-2 6.3
Dielectric Strength 0.600 kV/mm

@Thickness >=3.00 mm
15.2 kV/in

@Thickness >=0.118 in
24hr/23°C/50% RH+1hr/oil 90°C; Parallel; IEC 60245-1; IEC/EN 60893-2 6.1.3.2
2.00 kV/mm

@Thickness 3.00 mm
50.8 kV/in

@Thickness 0.118 in
24hr/23°C/50% RH+1hr/oil 90°C; Perpendicular; IEC 60245-1; IEC/EN 60893-2 6.1.3.1
Comparative Tracking Index 100 V

@Thickness 3.00 mm
100 V

@Thickness 0.118 in
IEC 60112; IEC/EN 60893-2 6.4