Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Elektro-Isola Etronit 201 MBM Phenolic/melamine, Paper Reinforcement, Grey/also other Colors, Sheets

Category Polymer , Thermoset , Phenolic
Manufacturer Elektro-Isola
Trade Name Etronit
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Elektro-Isola Etronit 201 MBM Phenolic/melamine, Paper Reinforcement, Grey/also other Colors, Sheets.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: This material is not standardized, but the base material is the same as Etronit 201 M. The surfaces consist of melamine, which ensures a scratch-resistant, tracking-resistant surface. The surfaces are grey as standard, but other colors can be selected from the color chart. The laminates are self-extinguishing over 8 mm in thickness.Applications: Used typically as front panels where and individual color is required.Information provided by Elektro-Isola
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
24hr/23°C/50% RH; ISO 1183-A; IEC/EN 60893-2 8.1
Water Absorption 1.6 %
1.6 %
24hr/50°C+24hr in water at 23°C,Test Specimen 50x50x3[mm]; ISO 62-1; IEC/EN 60893-2 8.2
Mechanical Properties Metric English Comments
Tensile Strength 90.0 MPa

@Thickness >=1.50 mm
13100 psi

@Thickness >=0.0591 in
24hr/23°C/50% RH; ISO 527; IEC/EN 60893-2 5.6
Modulus of Elasticity 10.0 GPa

@Thickness >=1.50 mm
1450 ksi

@Thickness >=0.0591 in
24hr/23°C/50% RH; ISO 178; IEC/EN 60893-2 5.2
Flexural Strength 120 MPa

@Thickness >=1.50 mm
17400 psi

@Thickness >=0.0591 in
24hr/23°C/50% RH; ISO 178; IEC/EN 60893-2 5.1
Compressive Strength 300 MPa

@Thickness >=5.00 mm
43500 psi

@Thickness >=0.197 in
24hr/23°C/50% RH; ISO 604; IEC/EN 60893-2 5.3
Shear Strength 35.0 MPa

@Thickness >=5.00 mm
5080 psi

@Thickness >=0.197 in
24hr/23°C/50% RH; IEC/EN 60893-2 5.5
Izod Impact, Notched (ISO) 3.30 kJ/m²

@Thickness >=5.00 mm
1.57 ft-lb/in²

@Thickness >=0.197 in
24hr/23°C/50% RH; ISO 180/2A; IEC/EN 60893-2 5.4.3
Thermal Properties Metric English Comments
Maximum Service Temperature, Inert 120 °C

@Thickness 0.000 mm,
Time 7.20e+7 sec
248 °F

@Thickness 0.000 in,
Time 20000 hour
IEC 60216; IEC/EN 60893-2 7.1
Flammability, UL94 V-0

@Thickness 8.00 mm
V-0

@Thickness 0.315 in
IEC/EN 60893-2 7.2; IEC 60695-11-10
Electrical Properties Metric English Comments
Insulation Resistance 5.00e+6 ohm

@Thickness >=3.00 mm
5.00e+6 ohm

@Thickness >=0.118 in
24hr/50°C+24h in water at 23°C; IEC 60167; IEC/EN 60893-2 6.3
Dielectric Strength 0.0400 kV/mm

@Thickness >=3.00 mm
1.02 kV/in

@Thickness >=0.118 in
24hr/23°C/50% RH+1hr/oil 90°C; Parallel; IEC 60245-1; IEC/EN 60893-2 6.1.3.2
Comparative Tracking Index 500 V

@Thickness 3.00 mm
500 V

@Thickness 0.118 in
IEC 60112; IEC/EN 60893-2 6.4