Material Notes:
Injection Grade Pellets. GMP # 002. Property values below represent typical values. Information provided by Engineered Plastics Corporation.
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
ASTM D792
Melt Flow 5.0 g/10 min
5.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 34.4 MPa
4990 psi
ASTM D638
Elongation at Break 10 %
10 %
ASTM D638
Flexural Modulus 2.07 GPa
300 ksi
ASTM D790
Izod Impact, Notched 2.70 J/cm
5.06 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 70.0 °C
158 °F
Annealed; ASTM Data
103 °C
217 °F
Unannealed; ASTM Data
Vicat Softening Point 104 °C
219 °F
ASTM D1525
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in