Ensinger DELRIN® 100AF Acetal Homopolymer, 13% PTFE filled (POM)

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Homopolymer, PTFE-Filled
Manufacturer Ensinger
Trade Name Delrin®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ensinger DELRIN® 100AF Acetal Homopolymer, 13% PTFE filled (POM).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ensinger’s DELRIN®100AF blend stock shapes are a 13% PTFE fiber filled homopolymer acetal. They offer an improved coefficient of friction, better lubricity, and improved wear characteristics over unfilled and PTFE powder filled acetals. This advanced acetal material uses a combination of PTFE fibers uniformly dispersed in Delrin acetal resin. The combination results in improved wear characteristics along with strength, toughness, dimensional stability and machinability. The materials exceptional wear properties and internal lubrication serves to reduce or eliminate the need for external lubricants. Ensinger can also produce a full strength 20% PTFE filled version.Excellent wear characteristicsSelf lubricatingLow coefficient of frictionMaximum unmodified toughnessSuperior load bearing characteristicsDELRIN®100AF is often used for applications such as bearing, bushings, cams and other antifriction devices that also require extra toughness.Information provided by Ensinger
Physical Properties Metric English Comments
Specific Gravity 1.50 g/cc
1.50 g/cc
ASTM D792
Density 1.49 g/cc
0.0540 lb/in³
ASTM D792
Water Absorption 0.12 %

@Time 86400 sec
0.12 %

@Time 24.0 hour
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell M 77
77
ASTM D785
Tensile Strength, Yield 54.25 MPa
7868 psi
ASTM D638
Elongation at Yield 10.3 %
10.3 %
ASTM D638
Tensile Modulus 2.36 GPa
342 ksi
1mm/min; ASTM D638
Izod Impact, Notched 0.534 J/cm
1.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 175 °C
347 °F
ASTM D3418
Maximum Service Temperature, Air 85.0 °C
185 °F
long term
149 °C
300 °F
intermittent
Deflection Temperature at 0.46 MPa (66 psi) 168 °C
334 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 118 °C
244 °F
ASTM D648
Flammability, UL94 HB
HB