Ensinger ENSIFONE® PSU (Polysulfone) - Extruded Products  (discontinued **)

Category Polymer , Thermoplastic , Polysulfone (PSU)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ensinger ENSIFONE® PSU (Polysulfone) - Extruded Products  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ENSIFONE is a transparent engineering plastic known for its chemical resistance, rigidity, high-temperature performance, and its ability to operate in an autoclave environment. ENSIFONE is FDA and NSF complaint and holds its excellent mechanical properties over a wide range of temperatures.Uses: ENSIFONE 's unique combination of chemical and hydrolytic resistance, high-temperature performance, good mechanical properties, and agency approvals make it an excellent choice for applications in the pharmaceutical, medical, food service equipment, semiconductor processing, and electronic equipment industries. Ensifone grades have been replaced by TecasonInformation supplied by Ensinger, Inc.
Physical Properties Metric English Comments
Density 1.24 g/cc
0.0448 lb/in³
ASTM D792
Water Absorption 0.30 %
0.30 %
24 hrs.; ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength, Ultimate 69.8 MPa
10100 psi
ASTM D638
Elongation at Break 50 - 100 %
50 - 100 %
ASTM D638
Tensile Modulus 2.48 GPa
360 ksi
ASTM D638
Flexural Yield Strength 106.2 MPa
15400 psi
ASTM D790
Flexural Modulus 2.70 GPa
392 ksi
1% Secant; ASTM D790
Izod Impact, Notched 0.690 J/cm
1.29 ft-lb/in
ASTM D256
Coefficient of Friction, Dynamic 0.37
0.37
40 psi, 50 fpm; ASTM D3702
Thermal Properties Metric English Comments
CTE, linear 55.8 µm/m-°C

@Temperature 20.0 °C
31.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Maximum Service Temperature, Air 141 °C
286 °F
Long Term
171 °C
340 °F
Short Term
Deflection Temperature at 0.46 MPa (66 psi) 181 °C
358 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 174 °C
345 °F
ASTM D648
Flammability, UL94 V-0
V-0
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Electrical Properties Metric English Comments
Electrical Resistivity 5.00e+16 ohm-cm
5.00e+16 ohm-cm
ASTM D257
Dielectric Constant 3.1

@Frequency 60 Hz
3.1

@Frequency 60 Hz
50% RH; ASTM D150
Dielectric Strength 16.5 kV/mm
419 kV/in
ASTM D149
Dissipation Factor 0.0010

@Frequency 60 Hz
0.0010

@Frequency 60 Hz
ASTM D150