Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ensinger ENSILON® 6/6 GF30 Extruded Nylon 6/6, 30% glass-fiber-reinforced (PA66)  (discontinued **)

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Extruded
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ensinger ENSILON® 6/6 GF30 Extruded Nylon 6/6, 30% glass-fiber-reinforced (PA66)  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ENSILON 6/6 GF30 is a 30% glass-fiber-reinforced nylon 6/6 material whose important properties include high tensile and flexural strength, stiffness, excellent heat deflection, and superior abrasion and wear resistance. While all ENSILON materials have high mechanical strength and superior resistance to wear and organic chemicals, ENSILON 6/6 GF30 has more than double the strength and stiffness of unreinforced nylons and a heat deflection temperature which approaches its melting point. Uses: ENSILON 6/6 GF30 has a balance of properties which make it an ideal material for metal replacement in applications such as automotive parts, industrial valves, railway tie insulators, and other industry uses whose design requirements include high strength, toughness, and weight reduction. Information supplied by Ensinger, Inc.Ensilon grades have been replaced by Tecamid
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
ASTM D792
Water Absorption 0.70 %
0.70 %
24 hrs.; ASTM D570
Water Absorption at Saturation 5.4 %

@Temperature 23.0 °C
5.4 %

@Temperature 73.4 °F
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell M 101
101
ASTM D785
Tensile Strength at Break 137.9 MPa
20000 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Yield Strength 268.9 MPa
39000 psi
ASTM D790
Flexural Modulus 8.30 GPa
1200 ksi
ASTM D790
Izod Impact, Notched 1.12 J/cm
2.10 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 21.6 µm/m-°C

@Temperature -20.0 - 200 °C
12.0 µin/in-°F

@Temperature -4.00 - 392 °F
ASTM D696
Maximum Service Temperature, Air 110 °C
230 °F
Long Term
241 °C
466 °F
Short Term
Deflection Temperature at 0.46 MPa (66 psi) 254 °C
489 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 250 °C
482 °F
ASTM D648
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
ASTM D257
Dielectric Constant 3.5

@Frequency 60 Hz
3.5

@Frequency 60 Hz
50% RH; ASTM D150
Dielectric Strength 20.9 kV/mm
531 kV/in
ASTM D149