Ensinger Hydex™ 202 Rigid Polyurethane (PU)

Category Polymer , Thermoplastic , Polyurethane, TP
Manufacturer Ensinger
Trade Name Hydex™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ensinger Hydex™ 202 Rigid Polyurethane (PU).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Hydex™ 202 is a totally rigid polyurethane resin that exhibits a broad range of chemical resistance, as well as superior impact and excellent mechanical properties. It can be used for any mechanical application that requires a combination of toughness, dimensional stability and chemical resistance. It has an ability to withstand chemical attack in a PH range from 2 to 14.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Water Absorption 0.21 %

@Time 86400 sec
0.21 %

@Time 24.0 hour
ASTM D570
Mechanical Properties Metric English Comments
Tensile Strength at Break 55.2 MPa
8000 psi
ASTM D638
Tensile Strength, Yield 62.1 MPa
9000 psi
ASTM D638
Elongation at Break 80 %
80 %
ASTM D638
Elongation at Yield 9.0 %
9.0 %
ASTM D638
Tensile Modulus 1.65 GPa
240 ksi
ASTM D638
Flexural Strength 82.7 MPa
12000 psi
ASTM D790
Flexural Modulus 1.93 GPa
280 ksi
ASTM D790
Izod Impact, Notched 5.34 J/cm
10.0 ft-lb/in
ASTM D256
Coefficient of Friction, Dynamic 0.22
0.22
SS counter surface
Coefficient of Friction, Static 0.26
0.26
SS counter surface
Thermal Properties Metric English Comments
CTE, linear 66.6 µm/m-°C
37.0 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 143 °C
290 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 138 °C
280 °F
ASTM D648
Vicat Softening Point 144 °C
292 °F
ASTM D1525